| 铸钢件准固态区域应力、应变数值模拟及热裂机制 |
| 贾宝仟;柳百成;王东涛 |
| 清华大学;北京;100084;清华大学;北京;100084;清华大学;北京;100084 |
|
| NUMERICAL SIMULATION OF STRESS-STRAIN IN CASTING STEEL DURING SOLIDIFICATION AND FORMATION MECHANISM OF HOT-TEARING |
| JIA Baoqian; LIU Baicheng; WANG Dongtao(Tsinghua University; Beijing 100084) |
引用本文:
贾宝仟;柳百成;王东涛. 铸钢件准固态区域应力、应变数值模拟及热裂机制[J]. 金属学报, 1997, 33(5): 504-508.
,
,
.
NUMERICAL SIMULATION OF STRESS-STRAIN IN CASTING STEEL DURING SOLIDIFICATION AND FORMATION MECHANISM OF HOT-TEARING[J]. Acta Metall Sin, 1997, 33(5): 504-508.
1林柏年.铸造流变学.哈尔滨:哈尔滨工业大学出版社,1991:102 2李德富,林柏年,阎永贵,安阁英.金属学报,1995;31:B389 |
|