|
|
|
| ZA27合金的高温拉伸性能 |
| 朱跃峰;曾大本;黄惠松;吴德海 |
| 中国科学院金属研究所;沈阳;110015;清华大学;北京;100084;清华大学;北京;100084;清华大学;北京;100084 |
|
| TENSILE PROPERTIES OF ALLOY ZA27 AT ELEVATED TEMPERATURES |
| ZHU Yuefeng (Institute of Metal Research; Chinese Academy of Sciences; Shenyang 110015); ZENG Daben; HUANG Huisong; WU Dehai (Tsinghua University; Beijing 100084) |
引用本文:
朱跃峰;曾大本;黄惠松;吴德海. ZA27合金的高温拉伸性能[J]. 金属学报, 1997, 33(5): 499-503.
,
,
,
.
TENSILE PROPERTIES OF ALLOY ZA27 AT ELEVATED TEMPERATURES[J]. Acta Metall Sin, 1997, 33(5): 499-503.
1 Gervais E,Levert H,Bess M.Trans Am Foundrymen's 1980;88:183 2Barber M J,Jones P E.Foundry Trade J,1980;148:114 3 Birch J.Mater Des,1990;11(2):83 4久保田耕平,二宫隆二,佐藤勉,尾城武司.铸物,1992;64:765 5曾松岩,段守坤,蒋祖龄,李庆春,孙阳.铸造技术,1991;(5):20 6李振镳.特种铸造及有色合金,1985;(2):10 7Walmag G,Lamberigts M,Coutsouradis D,洛阳工学院耐磨材料研究室译.第25届国际冶金年会译文选.北京:机械工业出版社,1992:9b |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|