| 含碳球团还原过程动力学及模型 |
| 黄典冰;杨学民;杨天钧;孔令坛 |
| 北京科技大学 |
|
| KINETICS AND MATHEMATICAL MODEL FOR REDUCTION PROCESS OF IRON ORE BRIQUETTE CONTAINING CARBON |
| HUANG Dianbing; YANG Xuemin; YANG Tianjun; KONG Lingtan (University of Science and Technology Beijing; Beijing 100083) |
引用本文:
黄典冰;杨学民;杨天钧;孔令坛. 含碳球团还原过程动力学及模型[J]. 金属学报, 1996, 32(6): 629-636.
,
,
,
.
KINETICS AND MATHEMATICAL MODEL FOR REDUCTION PROCESS OF IRON ORE BRIQUETTE CONTAINING CARBON[J]. Acta Metall Sin, 1996, 32(6): 629-636.
| 1YaoYK.MetallTrans,1971;2:14392McKeanWM.TransMetallSocAIME,1963;219:2193KawasakiE,SanscrainteJ,WalshTJ.AIchEJ,1962,8:484YaoYK.ChemEngSci1974;29:14355SihnHY,ChaubalPC.TransIronSteelInstJpn,1984;24:3876HuangDianbing,KongLingtan,LinZongcai.ActaMetallSin(EngEd),1994;7:577HuangDianbing,KongLingtan.10thProcessTechnologyConferenceProceedings,1992:4098于定年.钢铁,1985;5:489WilkeCR.ChemEngProg,1950;46:9510HuangDianbing,KongLingtan,LinZongcai,ActaMetallSin(EngEd)1993;68:227: |
|