| 热循环对TC4钛合金组织和机械性能的影响 |
| 耿洪滨;何世禹;雷廷权 |
| 哈尔滨工业大学材料科学与工程学院 |
|
| EFFECT OF THERMAL CYCLING ON MICROSTRUCTURE AND TENSILE PROPERTIES OF Ti-6Al-4V ALLOY |
| GENG Hongbin; HE Shiyu; LEI Tingquan (College of Materials and Engineering;Harbin Institute of Technology; Harbin 150001)(Manuscript received 1995-03-27; in revised form 1995-08-16) |
引用本文:
耿洪滨;何世禹;雷廷权. 热循环对TC4钛合金组织和机械性能的影响[J]. 金属学报, 1996, 32(1): 51-56.
,
,
.
EFFECT OF THERMAL CYCLING ON MICROSTRUCTURE AND TENSILE PROPERTIES OF Ti-6Al-4V ALLOY[J]. Acta Metall Sin, 1996, 32(1): 51-56.
| 1ToblerRL.ASTMSTP601,1976:3462吴运学.宇航材料及工艺,1992;4:623盛磊.宇航材料及工艺,1992;4:274金峰.宇航材料及工艺,1991;4:245邱惠中.宇航材料及工艺,1991;4:16EchigoyaJ.MaterSciEng,1991;63:Al417DaehnGS.ScrMetall,1988;22:10978VivekRatna.ScrMetall,1993;29:4679HEShiyu.ActaMetallSin(EngEd),1991,4A:55 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|