| 快速凝固Al-8.32Fe-3.4Ce合金中弥散合金相的TEM测定 |
| 张立春;何安强;叶恒强;张永昌;黄春 |
| 中国科学院金属研究所固体原子象开放实验室;北京科技大学新金属材料国家重点实验室;中国科学院金属研究所 |
|
| TEM STUDY OF DISPERSED INTERMETALLIC PHASES IN RAPIDLY SOLIDIFIED Al-8.32Fe-3.4Ce ALLOY |
| ZHANG Lichun;HE Anqiang;YE Hengqiang;ZHANG Yongchang;HUANG Chun(Laboratory of Atomic Imaging of Solids;Institute of Metal Research;Chinese Academy of Sciences;Shenyang 110015)(State Key Laboratory of Advanced Metallic Materials;University of Science and Technology Beijing;Beijing 100083)(Institute of Metal Research; Chinese Academy of Sciences;Shenyang 110015)(Manuscript received 1994-11-24;in revised form 1995-05-24) |
引用本文:
张立春;何安强;叶恒强;张永昌;黄春. 快速凝固Al-8.32Fe-3.4Ce合金中弥散合金相的TEM测定[J]. 金属学报, 1995, 31(11): 519-524.
,
,
,
,
.
TEM STUDY OF DISPERSED INTERMETALLIC PHASES IN RAPIDLY SOLIDIFIED Al-8.32Fe-3.4Ce ALLOY[J]. Acta Metall Sin, 1995, 31(11): 519-524.
| 1GriebB.BullAlloyPhaseDiagrams,1989;10:6692AyerR.MetallTrans,1988;19A:16453CarradM,GremM,PierantoniM.SciMetallMater,1991;25:9254KosugeH,MizukamiI.JJpnInstLightMet,1975,25:15BlankPJ.ActaCrystallogr,1955;A8:436AngersL.DissAbstrInt,1986;46:2887SkjerpeP.MetallTrans,1987;18A:1898YoungRMK,ClyneTW.ScrMetall,1981;15:1211> |
|