| GH30和GH34合金的蠕变-疲劳交互作用 |
| 王翔;周浩;孔庆平 |
| 中国科学院固体物理研究所 |
|
| CREEP-FATIGUE INTERACTION IN ALLOYS GH30 AND GH34 |
| WANG Xiang;ZHOU Hao;KONG Qingping(Institute of Solid State Physics;Chinese Academy of Sciences;Hefei)(Manuscript received 5 October;1993; in revised form 15 November;1993) |
引用本文:
王翔;周浩;孔庆平. GH30和GH34合金的蠕变-疲劳交互作用[J]. 金属学报, 1994, 30(5): 195-199.
,
,
.
CREEP-FATIGUE INTERACTION IN ALLOYS GH30 AND GH34[J]. Acta Metall Sin, 1994, 30(5): 195-199.
| 1RaiR.FlowandFractureatElevatedTemperatures,ASM,1985:Chapt6,72OhtaniR,OhnamiM,InonsT.HighTemperatureCreep-Fatigue,Elsevier19883LagneborgR,AttermoR.MetallTrans,1971;2:18214XieXS,SunXQ,GaoL,ChenGL,ChangFY,YuanZM.In:YanMGetal.eds.Procof5thIntConfonMechanicalBehaviourofMaterials,Vol.II.Oxford:Pergamon:1987;10375ChenGL.ChinJMetSciTechnol,1990;16:3916孔庆平,王翔,周浩,倪群慧.物理学报,1986;35:10917王翔,孔庆平,佟世华,江先美,任卫平.金属学报,1988;24:A1068WangDN,WangX,KongQP.MaterSciEng,1991;A142:1579WangX,NiQH,ZhouH,KongQP.MaterSciEng,1990;A123:20710WangX,ZhouH,NiQH,KongQP,ZhouNB.MaterSciEng,1989;A122:L911WangX,WangDN,KongQP.ScrMetallMater,1993;28:401 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|