| 碳对Fe-Cr-Mn合金高温氧化及磨损的影响 |
| 赵学增;邢建东;周庆德 |
| 哈尔滨电机厂;西安交通大学机械工程系;副教授;西安(710049);西安交通大学机械工程系 |
|
| INFLUENCE OF C ON OXIDATION AND WEAR OF Fe-Cr-Mn ALLOY AT HIGH TEMPERATURES |
| ZHAO Xuezeng;XING Jiandong;ZHOU Qingde Harbin Electric Machinery Plant; Xi'an Jiaotong University Correspondent associate professer; Department of Mechanical Engineering; Xi`an Jiaotong University; Xi`an 710049 |
引用本文:
赵学增;邢建东;周庆德. 碳对Fe-Cr-Mn合金高温氧化及磨损的影响[J]. 金属学报, 1992, 28(6): 65-70.
,
,
.
INFLUENCE OF C ON OXIDATION AND WEAR OF Fe-Cr-Mn ALLOY AT HIGH TEMPERATURES[J]. Acta Metall Sin, 1992, 28(6): 65-70.
| 1 Xing J D, Lu W H, Wang X T. Wear of Materials. Int Conf on Wear of Materials, New York: ASME, 1983: 45--61
2 Yan P, Zhou Q D. In: Ludema K C ed., Wear of Materials 1987, Vol. Ⅱ, Int Conf on Wear of Materials, Houston, Texas, April 5--9, 1987, New York: ASME, 1987: 743--752
3 Junyi S (Su J Y), Yadong J (Jia Y D). In: Ludema K C ed., Wear of Materials 1987, Vol. Ⅱ, Int conf on Wear of Materials, Houston, Texas, April 5--9, 1987, New York: ASME, 1987:666--671
4 邢建东,周庆德.摩擦磨损,1989;(1) :28--33
5 庄司雄次,秋山俊一郎,私市优,永利匡辅,星弘允.铁钢,1976;62:108--125
6 天野忠昭,矢岛圣使,斋藤安俊.日本金属学会志 1977;41:1074--1082
7 富土川尚男,村山顺一郎,藤野允克,诸石大司,庄司雄次.铁钢,1981;67:159--168
8 富士川尚男,村山顺一郎,藤野允克,诸石大司.铁钢,1981;67:169--177
9 山本章夫,泉(?)一,(?)原克俊,伊藤幸良.防食技术,1981;31:508--515
10 草开清志,士岐浩之,石黑隆羲,大冈耕之,铁钢,1988;74:871--878
11 邢建东,周庆德.西安交通大学学报,1990;24(4) :17--24
12 DesForges C D, Dancoisne P L. Environmental Degradation of High Temperature Materials. Proc Conf on Environmental Degradation of High Temperature Materials, Douglas, 1980: 5/22--5/37 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|