| 热处理对玻璃态Bi_(1.6)Pb_(0.4)Sr_(1.9)Ca_2Cu_(3.1)O_y正电子湮没特性的影响 |
| 张宏 |
| 中国科学院上海冶金研究所;副研究员;上海(200050)中国科学院上海冶金研究所 |
|
| EFFECTS OF HEAT TREATMENT ON POSITRON ANNIHILATION OF GLASSY BPSCCO |
| ZHANG Hong Shanghai Institute of Metallurgy; Academia Sinica |
引用本文:
张宏. 热处理对玻璃态Bi_(1.6)Pb_(0.4)Sr_(1.9)Ca_2Cu_(3.1)O_y正电子湮没特性的影响[J]. 金属学报, 1992, 28(2): 77-81.
.
EFFECTS OF HEAT TREATMENT ON POSITRON ANNIHILATION OF GLASSY BPSCCO[J]. Acta Metall Sin, 1992, 28(2): 77-81.
1 Komatsu T, Sato R, Hirose C, Matusita K, Yamashita T. Jpn J Appl Phys, 1988; 27: L2293 2 Ibara Y, Nasu H, Imara T, Osaka Y. Jpn J Appl Phys, 1989; 28: L37 3 Sato R, Komatsu T, Matusita K, Yamashita T. Jpn J Appl Phys, 1989; 28: L583 4 Abe Y, Hosono H, Hosoe M, Iwase J, Kubo Y. Appl Phys Lett, 1988; 53: 1341 5 LeBeau S E, Righi J, Ostenso J E, Sanders S C, Finnemore D K. Appl Phys lett, 1988; 55: 292
6 Kirkengaard P, Edlrup M. Comput Phys Commun, 1972: 3: 240 7 Paul A, Sigru R M, Dauwe C, Dorikens-Vanpraet L, Dorikens M. J Phys C: Solid State Phys, 1974; 7: 2180 8 Singh Y P, West R N, Paul A. J Phys C: Solid State Phys, 1976; 9: 305 9 Yavari A R, Lejay P. J Cryst Growth, 1988; 91: 290 10 Usmar S G, Rawson H, West R N. In: Coleman P G, Sharma S C, Diana L M eds., Positron Annihilation, Proc 6th Int Conf, The University of Texas at Arlington, April 3--7, 1982, Amsterdam: North-Holland, 1983: 660 11 Shiotani N. In: Coleman P G, Sharma S C, Diana L M eds., Positron Annihilation, Proc 6th Int Conf, The University of Texas at Arlington, April 3--7, 1982, Amsterdam: North-Holland, 1983: 561 12 Morse P, Corbel C. In: Brandt W, Dupasquier A eds., Positron Solid-State Physics, Amsterdam: North-Holland, 1983: 679 |
|