| 退火变脆Fe_(75)Si_(10)B_(15)金属玻璃的脆韧性转变 |
| 王隆保 |
| 中国科学院金属研究所;快速凝固非平衡合金国家重点实验室副研究员;沈阳(110015)中国科学院金属研究所 |
|
| BRITTLE-DUCTILE TRANSITION OF ANNEAL-EMBRITTLED Fe_(75)Si_(10)B_(15) METALLIC GLASS |
| WANG Longbao State Key Laboratory of Rapidly Solidified Non-Equilibrium Alloys; Institute of Metal Research; Academia Sinica; Shenyang; |
引用本文:
王隆保. 退火变脆Fe_(75)Si_(10)B_(15)金属玻璃的脆韧性转变[J]. 金属学报, 1992, 28(2): 64-70.
.
BRITTLE-DUCTILE TRANSITION OF ANNEAL-EMBRITTLED Fe_(75)Si_(10)B_(15) METALLIC GLASS[J]. Acta Metall Sin, 1992, 28(2): 64-70.
1 Gerling R, Schimansky F P, Wagner R. Acta Metall, 1987; 35: 1001. 2 Davies H A, Small C J. J Less-Common Met, 1988; 140: 185 3 Chen H S, Inoue A, Masumoto T. J Mater Sci, 1985; 20: 2417 4 Donovan P E, Stobbs W M. Acta Metall, 1981; 29: 1419 5 Li J C M. In: Masumoto T, Suzuki K eds., Rapidly Quenched Metals 4, Vol. Ⅱ, Proc 4th Int Conf Rapidly Quenched Metals, Sendai, Augest 24--28, 1981, The Japan Inst Metals, 1982: 1335 6 Eckert J, Schultz L, Hellstern E, Urban K. J Appl Phys, 1988; 64: 3224 7 Trudeau M L, Schulz R. Phys Rev lett, 1990; 64: 99 8 Steif P S, Spaepen F, Hutchinson J W. Acta Metall, 1982; 30: 44 |
|