| 316不锈钢热照射疲劳中的硬化行为 |
| 颜世春;奥田重雄;水林博 |
| 中国科学院固体物理研究所;副研究员;合肥市(230031)中国科学院固体物理研究所;日本筑波大学物质工学系;日本筑波大学物质工学系 |
|
| HARDENING BEHAVIOUR OF STAINLESS STEEL 316 DURING FATIGUE WITH THERMAL PULSE |
| YAN Shichun;OKUDA Shigeo;MIZUBAYASHI Haka Institute of Solid State Physics; Academia Sinica; Hefei; Institute of Materials Science; University of Tsukuba; Japan |
引用本文:
颜世春;奥田重雄;水林博. 316不锈钢热照射疲劳中的硬化行为[J]. 金属学报, 1992, 28(2): 39-42.
,
,
.
HARDENING BEHAVIOUR OF STAINLESS STEEL 316 DURING FATIGUE WITH THERMAL PULSE[J]. Acta Metall Sin, 1992, 28(2): 39-42.
1 Mizubayashi H, Okuda S, Nakagome K, Shibuki H, Seki S. Trans Jpn Inst Met, 1984; 25: 257 2 Shibuki H, Mizubayashi H, Okuda S. Trans Jpn Inst Met, 1986: 27: 673 3 Mizubayashi H, Ikezaki K, Okuda S, Roberts J M. Trans Jpn Inst Met, 1987; 28: 463 4 颜世春,水林博,奥田重雄.核科学与工程,待发表 5 Okuda S, Mizubayashi H, Tago Y. J Phys E: Sci Instrum, 1984; 17: 111 |
|