| 快速凝固Al-Li-Mg-Zr合金粉末粒度对组织和性能影响 |
| 于桂复;何军舫;李庆春 |
| 北京航空材料研究所;中国科学院金属研究所;哈尔滨工业大学 |
|
| EFFECT OF POWDER SIZE ON MICROSTRUCTURE AND PROPERTIES OF RAPIDLY SOLIDIFIED Al-Li-Mg-Zr ALLOY |
| YU Guifu;HE Junfang;LI Qingchun Beijing Institute of Aeronautical Materials; Institute of Metal Research; Academia Sinica; Shenyang; Harbin Institute of Technology |
引用本文:
于桂复;何军舫;李庆春. 快速凝固Al-Li-Mg-Zr合金粉末粒度对组织和性能影响[J]. 金属学报, 1992, 28(1): 34-38.
,
,
.
EFFECT OF POWDER SIZE ON MICROSTRUCTURE AND PROPERTIES OF RAPIDLY SOLIDIFIED Al-Li-Mg-Zr ALLOY[J]. Acta Metall Sin, 1992, 28(1): 34-38.
1 Tietz T E, Palmer I G. In: Chin G Y ed., Advances in Powder Technology, Ohio: ASM, 1982: 189 2 Kang S, Grant W J. In: Starke E A Jr., Sanders T H Jr. eds., Aluminum-Lithium Alloys Ⅱ, Proc Second In Al-Li Conf, Monterey, California, 12-14 April 1983, New York: AIME, 1983 3 Meschter P J, Lederich R J, O'Neal J E. In: Baker C, et al eds., Aluminum-Lithium Alloys Ⅲ, Proc 3th Int Al-Li Conf. University of Oxford, July, 1985 London: The Institute of Metals, 1986 4 Kim Y W, Froes F H. In: Froes F H, Savage S J eds, Proc of Structural Metals by Rapid Solidification. Proc of a Seven Session Symposium on Enhanced Properties in Structural Metals Via Rapid Solidification, Orlando, Florida, 6-9 October, 1986, New York: ASM, 1987: 309--321 5 于桂复.颜鸣皋.余正华.轻质结构材料-Al-Li合金,北京航空材料研究所内部资料,1987 6 何军舫.快速凝固Al-Li-Mg-Zr粉末及合金组织和性能的研究,哈尔滨工业大学硕士学位论文,1990 |
|