|
|
|
| Bi-Pb-Tl三元系相图 |
| 车广灿;M.ELLNER |
| 中国科学院物理研究所;副研究员;德国马普金属所 |
|
| PHASE DIAGRAM OF Bi-Pb-Tl TERNARY SYSTEM |
| CHE Guangcan Institute of Physics; Academia Sinica; Beijing; ELLNER M. Max-Planck-Institut for Metallforschung; Stuttgart; Germany |
引用本文:
车广灿;M.ELLNER. Bi-Pb-Tl三元系相图[J]. 金属学报, 1991, 27(6): 152-154.
,
.
PHASE DIAGRAM OF Bi-Pb-Tl TERNARY SYSTEM[J]. Acta Metall Sin, 1991, 27(6): 152-154.
1 Massalski T B. Binary Alloy Phase Diagrams. American Society for Metals, 1986 2 Hansen M. Constitotion of Binary Alloys. London: McGraw-Hill, 1958 3 Coles B R. IBM J Res Dev, 1962; 6: 68 4 Predel B. Schwermann W. Z Metallk, 1970; 61: 585 Predel B, Schwermann W. Z Metallk, 1971; 62: 517 5 Claeson T, Ostklint D. Acta Mctall, 1974; 22: 759 6 Matsuda T. Trans Jpn Inst Met, 1979; 20: 742 7 1950; 74: 935 8 Villars P. Pearson's Handbook of Crystallographic Data for Intermetallic Phases, American Society for Metals, 1985 9 Pearson W B. Handbook of Lattice Spacings and Structures of Metals, 1967 10 Tang Y C. Acta Crystallogr, 1952; 5: 99 11 Ellner M. J Less-Common Met, 1979; 68: 99 12 Kleme T. J Phys Chem, 1963; 38: 298 |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|