| 非晶态Pd-Y-Si合金的电子结构 |
| 骆梅青;陈念贻;俞志中;宁远涛;周新铭 |
| 中科院上海冶金研究所;中科院上海冶金研究所;研究员;上海(200050);上海测试中心;昆明贵金属研究所;昆明贵金属研究所 |
|
| ELECTRONIC STRUCTURE OF AMORPHOUS Pd-Y-Si ALLOY |
| LUO Meiqing;CHEN Nianyi;YU Zhizhong;NING Yuantao;ZHOU Xinming Shanghai Institute of Metallurgy; Academia Sinica Shanghai Institute of Testing Technics Kunming Institute of Precious Metals CHEN Nianyi; professor; Shanghai Institute of Metallurgy; Academia Sinica; 200050 Shanghai |
引用本文:
骆梅青;陈念贻;俞志中;宁远涛;周新铭. 非晶态Pd-Y-Si合金的电子结构[J]. 金属学报, 1989, 25(5): 147-148.
,
,
,
,
.
ELECTRONIC STRUCTURE OF AMORPHOUS Pd-Y-Si ALLOY[J]. Acta Metall Sin, 1989, 25(5): 147-148.