高温合金中碳化物的初生形貌与晶体结构的关系 |
刘林;傅恒志;史正兴 |
西北工业大学;西北工业大学;西北工业大学 |
|
RELATIONSHIP BETWEEN PRIMARY MORPHOLOGY AND CRYSTAL STRUCTURE OF MC CARBIDES PRECIPITATED IN SUPERALLOYS |
LIU Lin;FU Hengzhi;SHI Zhengxing Northwestern Polytechnical University; Xi'an |
引用本文:
刘林;傅恒志;史正兴. 高温合金中碳化物的初生形貌与晶体结构的关系[J]. 金属学报, 1989, 25(4): 48-53.
,
,
.
RELATIONSHIP BETWEEN PRIMARY MORPHOLOGY AND CRYSTAL STRUCTURE OF MC CARBIDES PRECIPITATED IN SUPERALLOYS[J]. Acta Metall Sin, 1989, 25(4): 48-53.
1 傅恒志,史正兴,方晓华,薛玉芳,孙承业.特种铸造及有色金属,1983;(3) :16 2 刘林,傅恒志,史正兴.航空学报,1986;7:181 3 傅恒志,刘林,方晓华,史正兴,薛廷禄.西北工业大学学报,1987;5:279 4 Higashi H. Takahashi Y, Atoda T. J Cryst Growth. 1976; 33: 207 5 刘林.西北工业大学博士论文,1988 6 Samsonov G V. Plenum Press Handbook of High-Temperature Materials №2, Properties Index, New York: Plenum Press, 1964: 44 7 Donnay J D H, Harker D. Am Mineral, 1937; 22: 446 8 Laue M V. In: Schneer C J ed, Crystal Form and Structure, Pennsylvania: Hutchinson & Ross, 1977: 141 9 Hartman P, Perdok W G. Acta Crystallogr, 1955; 8: 49, 521 10 Hartman P. In: Hartman P ed, Crystal Growth: an Introduction, Amsterdam: North-Holland, 1973: 367 11 Hartman P, Bennema P. J Cryst Growth, 1980; 49: 145 12 Bennema P, Gilmer G H. In: Hartman P ed, Crystal Growth: an Introduction, Amsterdam: North-Holland, 1973: 263 13 刘林.傅恒志.材料科学讲展.待发表 14 Smith J V. Geometrical and Structual Crystallography, New York: John & Sons, 1982: 373o |
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|