| 金属学报 DOI: 10.11900/0412.1961.2026.00101 |
|
|
|
| 磁控溅射-热处理过程中Nb3Sn薄膜的界面演变与生长机制 |
| 巩晓乐1,2, 高勇2, 陈岩1,2, 信纪军2, 杨清1,2, 尹圆圆2, 赵红运1, 王维1,2 |
1 中色创新研究院(天津)有限公司 天津 300393
2 松山湖材料实验室 东莞 523000
|
|
Microstructural Evolution and
Growth Mechanisms of Nb3Sn Thin Films During Magnetron Sputtering
and Heat Treatment
|
GONG Xiaole 1,2, GAO Yong 2,
CHEN Yan 1,2, XIN Jijun 2, YANG Qing 1,2, YIN
Yuanyuan 2, ZHAO Hongyun 1, WANG Wei 1,2
|
1 China Nonferrous Metals Innovation
Research Institute (Tianjin) Co. Ltd., Tianjin 300393, China
2 Songshan Lake Materials
Laboratory, Dongguan 523000, China
|