| 金属学报 DOI: 10.11900/0412.1961.2025.00112 |
|
|
|
| 微合金化元素对偏晶合金两液相间界面能影响 |
| 张丽丽1,郜冰1,2,江鸿翔1,赵雷3,赵九洲1,何杰1 |
1 中国科学院金属研究所 师昌绪先进材料创新中心 沈阳 110016
2 东北大学 材料科学与工程学院 沈阳 110819
3 辽宁石油化工大学 机械工程学院 抚顺 113001
|
|
| EFFECT OF MICRO-ALLOYING ELEMENT ON INTERFACIAL ENERGY BETWEEN TWO LIQUID PHASES IN A MONOTECTIC ALLOY |
ZHANG
Lili 1, GAO Bing 1,2, JIANG Hongxiang 1, ZHAO
Lei 3, ZHAO Jiuzhou 1, HE Jie 1
|
1 Shi-changxu Innovation
Center for Advanced Materials, Institute of Metal Research, Chinese Academy
of Sciences, Shenyang 110016, China
2 School of Materials Science and
Engineering, Northeastern University, Shenyang 110819, China
3 School of Mechanical Engineering,
Liaoning Petrochemical University, Fushun 113001, China
|
引用本文:
张丽丽 郜冰 江鸿翔 赵雷 赵九洲 何杰. 微合金化元素对偏晶合金两液相间界面能影响[J]. 金属学报, DOI: 10.11900/0412.1961.2025.00112.
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|