| 汽车车身用Al-Mg-Si-Cu合金薄板应变强化行为的研究 |
| 田妮; 赵刚; 左良; 刘春明 |
| 东北大学材料各向异性与织构教育部重点实验室; 沈阳 110819 |
|
| STUDY ON THE STRAIN HARDENING BEHAVIOR OF Al-Mg-Si-Cu ALLOY SHEET FOR AUTOMOTIVE BODY |
| TIAN Ni; ZHAO Gang; ZUO Liang; LIU Chunming |
| Key Laboratory for Anisotropy and Texture of Materials (Ministry of Education); Northeastern University; Shenyang 110819 |
引用本文:
田妮 赵刚 左良 刘春明 . 汽车车身用Al-Mg-Si-Cu合金薄板应变强化行为的研究[J]. 金属学报, 2010, 46(5): 613-617.
,
,
,
.
STUDY ON THE STRAIN HARDENING BEHAVIOR OF Al-Mg-Si-Cu ALLOY SHEET FOR AUTOMOTIVE BODY[J]. Acta Metall Sin, 2010, 46(5): 613-617.
| [1] Saito M, Iwasuki S, Yasunaga K, Andoh K. JSAE Rev, 2000; 21: 511
[2] Miller W S, Zhuang L, Bottema J, Wittebrood A J, Smet P D, Haszler A, Vieregge A. Mater Sci Eng, 2000; A280: 37
[3] Carle D, Blount G. Mater Des, 1999; 20: 267
[4] C´aceres C H. Mater Des, 2009; 30: 2813
[5] WanM,Yang Y Y, Li S B. J Mater Process Technol, 2001; 116: 189
[6] Barlat F, Berm J C. Int J Plast, 2003; 19: 1297
[7] Yu Z Q, Zhao Y X, Lin Z Q. Chin J Nonferrous Met, 2004; 14: 1689
(于忠奇, 赵亦希, 林忠钦. 中国有色金属学报, 2004; 14: 1689)
[8] Zhao Y X, Yu Z Q. Mater Sci Technol, 2007; 15: 98
(赵亦希, 于忠奇. 材料科学与工艺, 2007; 15: 98)
[9] Song Y Q, Guan Z P, Ma P K, Song J W. Acta Metall Sin, 2006; 42: 673
(宋玉泉, 管志平, 马品奎, 宋家旺. 金属学报, 2006; 42: 673)
[10] Troeger L P, StarkeJr E A. Mater Sci Eng, 2000; A277: 102
[11] O’Brien M J, Bremen H F, Furukawa M, Horita Z, Langdon T G. Mater Sci Eng, 2007; A456: 236
[12] Ludwigson D C. Metall Trans, 1971; 2: 2825
[13] Mannan S L, Samuel K G, Rodriguez P. Scr Metall, 1982; 16: 255
[14] Sun L, Zhang Q C, Jiang H F. Acta Metall Sin, 2006; 42: 1248
(孙亮, 张青川, 江慧丰. 金属学报, 2006; 42: 1248)
[15] Jiang H F, Zhang Q C, Wu X P, Fan J H. Scr Mater, 2006; 54: 2041
[16] Abbadi M, H¨ahner P, Zeghloul A. Mater Sci Eng, 2002; A337: 194 |
|