| E690高强钢在SO2污染海洋大气环境中的应力腐蚀行为研究* |
马宏驰1,杜翠薇1,刘智勇1( ),郝文魁1,李晓刚1,2,刘超1 |
1 北京科技大学腐蚀与防护中心教育部腐蚀与防护重点实验室, 北京 100083
2 中国科学院宁波材料技术与工程研究所, 宁波 315201 |
|
| STRESS CORROSION BEHAVIORS OF E690 HIGH-STRENGTH STEEL IN SO2-POLLUTED MARINE ATMOSPHERE |
Hongchi MA1,Cuiwei DU1,Zhiyong LIU1( ),Wenkui HAO1,Xiaogang LI1,2,Chao LIU1 |
1 Key Laboratory for Corrosion and Protection, Ministry of Education, Corrosion and Protection Center, University of Science and Technology Beijing, Beijing 100083, China
2 Ningbo Institute of Material Technology & Engineering, Chinese Academy of Sciences, Ningbo 315201, China |
引用本文:
马宏驰, 杜翠薇, 刘智勇, 郝文魁, 李晓刚, 刘超. E690高强钢在SO2污染海洋大气环境中的应力腐蚀行为研究*[J]. 金属学报, 2016, 52(3): 331-340.
Hongchi MA,
Cuiwei DU,
Zhiyong LIU,
Wenkui HAO,
Xiaogang LI,
Chao LIU.
STRESS CORROSION BEHAVIORS OF E690 HIGH-STRENGTH STEEL IN SO2-POLLUTED MARINE ATMOSPHERE[J]. Acta Metall Sin, 2016, 52(3): 331-340.
| [1] | Han E-H, Chen J M, Su Y J, Liu M.Mater China, 2014; 33(2): 65 | | [1] | (韩恩厚, 陈建敏, 宿彦京, 刘敏. 中国材料进展, 2014; 33(2): 65) | | [2] | Nishikata A, Ichihara Y, Hayashi Y, Tsuru T.J Electrochem Soc, 1997; 144: 1244 | | [3] | Zhong X K, Zhang G A, Qiu Y B, Chen Z Y, Guo X P, Fu C Y. Corros Sci, 2013; 66: 14 | | [4] | Qiao L J, Luo J L, Mao X.Corrosion, 1998; 54: 115 | | [5] | Dmytrakh I M, Smiyan O D, Syrotyuk A M, Bilyy O L.Int J Fatigue, 2013; 50: 26 | | [6] | Gu B, Luo J, Mao X.Corrosion, 1999; 55: 96 | | [7] | Li M C, Cheng Y F.Electrochim Acta, 2007; 52: 8111 | | [8] | Chen W J, Hao L, Dong J H, Ke W, Wen H L.Acta Metall Sin, 2014; 50: 802 | | [8] | (陈文娟, 郝龙, 董俊华, 柯伟, 文怀梁. 金属学报, 2014; 50: 802) | | [9] | Wang C, Wang Z Y, Ke W.Acta Metall Sin, 2008; 44: 729 | | [9] | (汪川, 王振尧, 柯伟. 金属学报, 2008; 44: 729) | | [10] | Chen W J, Hao L, Dong J H, Ke W.Corros Sci, 2014; 83: 155 | | [11] | Wang J H, Wei F I, Chang Y S, Shih H C.Mater Chem Phys, 1997; 47: 1 | | [12] | Nishimura R, Shiraishi D, Maeda Y.Corros Sci, 2004; 46: 225 | | [13] | Zheng C B, Huang Y L, Wang X, Sun G J, Pan L Z.Mater Prot, 2011; 44(5): 34 | | [13] | (郑传波, 黄彦良, 王旭, 孙广杰, 潘立志. 材料保护, 2011; 44(5): 34) | | [14] | Zheng C B.PhD Dissertation, Institute of Oceanography, Chinese Academy of Sciences, Qingdao, 2008 | | [14] | (郑传波. 中国科学院海洋研究所博士学位论文, 青岛, 2008) | | [15] | Xiong X Q, Xiong W M, Chen Y J, Sun X Z.Jiangxi Metall, 2012; 32(6): 21 | | [15] | (熊小强, 熊文名, 陈英俊, 孙熙钟. 江西冶金, 2012; 32(6): 21) | | [16] | Zhang J, Cai Q W, Wu H B, Fan X H, Zhang M J.J Univ Sci Technol Beijing, 2012; 34: 657 | | [16] | 张杰, 蔡庆伍, 武会宾, 樊学华, 张明洁. 北京科技大学学报, 2012; 34: 657) | | [17] | Wu B, Cai Q W, Zhang J, Wu H B.Heat Treat Met, 2011; 36(3): 26 | | [17] | (武博, 蔡庆伍, 张杰, 武会宾. 金属热处理, 2011; 36(3): 26) | | [18] | Hao W K.PhD Dissertation, University of Science and Technology Beijing, 2015 | | [18] | (郝文魁. 北京科技大学博士学位论文, 2015) | | [19] | Ma Y T, Li Y, Wang H F.Corros Sci, 2009; 51: 997 | | [20] | Hao L, Zhang S X, Dong J H, Ke W.Corros Sci, 2012; 58: 175 | | [21] | Collazo A, Novoa X R, Pérez C, Puga B.Electrochim Acta, 2008; 53: 7565 | | [22] | Zhang Q C, Wu J S, Wang J J, Zheng W L, Chen J G, Li A B.Mater Chem Phys, 2003; 77: 603 | | [23] | Castaño J G, Botero C A, Restrepo A H, Agudelo E A, Correa E, Echeverría F.Corros Sci, 2010; 52: 216 | | [24] | Hao L, Zhang S X, Dong J H, Ke W. Corros Sci, 2012; 59: 270 | | [25] | Akiyama E, Li S, Shinohara T, Zhang Z, Tsuzaki K.Electrochim Acta, 2011; 56: 1799 | | [26] | Akiyama E, Matsukado K, Wang M, Tsuzaki K.Corros Sci, 2010; 52: 2758 | | [27] | Tsuru T, Huang Y L, Ali M R, Nishikata A.Corros Sci, 2005; 47: 2431 | | [28] | Antony H, Perrin S, Dillmann P, Legrand L, Chaussé A.Electrochim Acta, 2007; 52: 7754 | | [29] | Zhou Y L, Chen J, Liu Z Y.J Iron Steel Res, 2013; 20: 66 | | [30] | Tamura H.Corros Sci, 2008; 50: 1872 | | [31] | Kamimura T, Hara S, Miyuki H, Yamashita M, Uchida H.Corros Sci, 2006; 48: 2799 | | [32] | Dillmann P, Mazaudier F, Hoerle S.Corros Sci, 2004; 46: 1401 | | [33] | Yamashita M, Miyuki H, Matsuda Y, Nagano H, Misawa T.Corros Sci, 1994; 36: 283 | | [34] | Singh D D, Yadav S, Saha J K.Corros Sci, 2008; 50: 93 | | [35] | Allam I M, Arlow J S, Saricimen H.Corros Sci, 1991; 32: 417 |
|
|