    					| 双剪切试样用于短纤维金属基复合材料的蠕变响应研究 | 
  					 
  					  										
						| 岳珠峰;胡卫兵;吕震宙 | 
					 
															
					| 西北工业大学工程力学系;西安 710072 | 
					 
										
						 | 
					 
   										
    					| Application of the Double Shear Creep Specimens on the Fiber-Reinforced Metal Matrix Composites | 
  					 
  					  					  					
						| YUE Zhufeng; HU Weibing; LU Zhenzhou | 
					 
															
						| Department of Engineering; Mechanics; Northwestern Polytechnical University; Xi’710072 | 
					   
									 
				
				引用本文: 
				
								岳珠峰; 胡卫兵; 吕震宙                                                                                                                                                                                                                                           . 双剪切试样用于短纤维金属基复合材料的蠕变响应研究[J]. 金属学报, 2003, 39(1): 104-108       .	
																												 																				 ,
																								 ,
																												 . 
				Application of the Double Shear Creep Specimens on the Fiber-Reinforced Metal Matrix Composites[J]. Acta Metall Sin, 2003, 39(1): 104-108       .	                                                        				  
				
				
					
						
							
								
									
									
									
									
									 
          
          
            
                         
            
									            
									                
																														  
																  [1] Dong M, Schmander S. Comput Mater Sci, 1996; (5) : 53 [2] Phillips J, Staubach M, Skrotzki B, Eggeler G. Mater SciEng, 1997; A234-236: 401 [3] Cheng C, Aravas N. Int J Solid Struct, 1997; 34: 4173 [4] Nam H W, Han K S. Metall Mater Trans A, 1998; 29:1983 [5] Cseh G, Bar J, Gudladt H J, Lendvai J, Juhasz A. MaterSci Eng, 1999; A272: 145  [6] Yue Z F, Probst-Hem M, Eggeler G. Mater High Temp, 2000; 17: 449 [7] Mayr C, Eggeler G, Webster G A, Peter G. Mater Sci Eng A, 1995;199: 121 [8] Peter G, Probst-Hein M, Koolbe M, Neuking K, Eggeler G. Mater Sci Technol, 1997; 28, 457 [9] Yue Z F. Alexander von Humboldt Foundation (AvH) Report, 2000 [10] Kaustrater G, Yawny A, Schurhoff J, Skrotzki B, Eggeler G, Stockhert B. In: Parker J D ed. Creep & Fracture on Engineering Materials & Structures, Proceedings of the 9th International Conference, Swansea, 2001; April: 1 | 
															   
																													 
									             
									           
             
			            			 
			 
             
												
											    	
											        	 | 
											        	Viewed | 
											         
													
											        	 | 
											        	 | 
											         
											      	
												         | 
												        
												        	Full text 
												          	
												         | 
											        	
												        	
												        	 
												        	
												          	 
												          	
												          	
														 | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        
												        	Abstract 
												          	
														 | 
												        
															
															 
															
															
												         | 
													 
													
												         | 
												         | 
													 
													
												         | 
												        Cited  | 
												        
												        	
												         | 
													 
													
												         | 
												         | 
												         | 
													 
													
													    |   | 
													    Shared | 
													       | 
												  	 
												  	
													     | 
													     | 
													     | 
											  		 
											  		
													    |   | 
													    Discussed | 
													       | 
												  	 
											 
											 
             
           
      
									
									
		
									
									
									
									
									
									 | 
								 
							 
						 | 
					 
				 
			
		 |