| TOUGHENING AND STRENGTHENING OF Al_2O_3 CERAMICS THROUGH NANO-Al_2O_3 ADDITION |
| LI Guanghai;JIANG Anquan;ZHANG Lide (Institute of Solid State Physics; Chinese Academy of Sciences; Hefei 230031)(Manuscript received 1995-12-27; in revised form 1996-08-12) |
|
Cite this article:
LI Guanghai;JIANG Anquan;ZHANG Lide (Institute of Solid State Physics; Chinese Academy of Sciences; Hefei 230031)(Manuscript received 1995-12-27; in revised form 1996-08-12). TOUGHENING AND STRENGTHENING OF Al_2O_3 CERAMICS THROUGH NANO-Al_2O_3 ADDITION. Acta Metall Sin, 1996, 32(12): 1285-1288.
|
|
|
Abstract Nano-Al2O3 powders processed by the hydrolysis technique of pure Al sheet after activation were added into Al2O3 ceramics.The results indicated that the nano-Al2O3 addition can increase not only the sinterability of the Al2O3 ceramics, but the fracture toughness and bending strength as well, and this kind of increase can be obtained only when the grain size of the added nano-Al2O3 is small enough, for example,37 nm.
|
|
|
| 1HahnH.NanostructMater,1993;2:2512GleiterH.ProgMaterSci,1991;33:2233JangJSC,KochCC.ScrMetallMater,1990;24:15994HofterHJ,AverbackRS.ScrMetallMater,1990;24:24015SuryanarayanaC.IntMaterRev,1995;40:416AnddevskiRA.JMaterSci,1994;29:6147李广海,费广涛,张立德.'95秋季中国材料研讨会论文集.北京,1996:488张立德,牟季美.纳米材料学.沈阳:辽宁科学技术出版社,19949DavidgeRW,GreenTJ.JMaterSci,1968;3:629r |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|