| EFFECTS OF RE ON PROCESS OF COMPOSITE PLATING AND PROPERTIES OF COATING |
| GUO Zhongcheng(Department of Metallurgy; Kunming Institute of Technology;Kunming 650093)(Manuscript received 1995-09-20; in revised form 1995-12-05) |
|
Cite this article:
GUO Zhongcheng(Department of Metallurgy; Kunming Institute of Technology;Kunming 650093)(Manuscript received 1995-09-20; in revised form 1995-12-05). EFFECTS OF RE ON PROCESS OF COMPOSITE PLATING AND PROPERTIES OF COATING. Acta Metall Sin, 1996, 32(5): 516-520.
|
|
|
Abstract The effects of RE on the process of electroplating and electroless plating and properties of coating have been studied. The results show that SiC content, hardness and wear resistance of the composite coatings increase obviously when a few RE are added in the bath.
|
|
Received: 18 May 1996
|
| 1ThomaM.PlatSurfFin,1984;76:532MatsufumiT.J METFinishSocJpn,1987;38:5673VestGE.MetalFinishing,1967;65:824郭忠诚.有色金属(季刊),1994:46:675郭忠诚,材料保护,1991:24:15 |