EFFECTS OF RE ON PROCESS OF COMPOSITE PLATING AND PROPERTIES OF COATING
GUO Zhongcheng(Department of Metallurgy; Kunming Institute of Technology;Kunming 650093)(Manuscript received 1995-09-20; in revised form 1995-12-05)
Cite this article: 

GUO Zhongcheng(Department of Metallurgy; Kunming Institute of Technology;Kunming 650093)(Manuscript received 1995-09-20; in revised form 1995-12-05). EFFECTS OF RE ON PROCESS OF COMPOSITE PLATING AND PROPERTIES OF COATING. Acta Metall Sin, 1996, 32(5): 516-520.

Download:  PDF(304KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The effects of RE on the process of electroplating and electroless plating and properties of coating have been studied. The results show that SiC content, hardness and wear resistance of the composite coatings increase obviously when a few RE are added in the bath.
Key words:  rare earth      electroplating      electroless plating     
Received:  18 May 1996     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1996/V32/I5/516

1ThomaM.PlatSurfFin,1984;76:532MatsufumiT.J METFinishSocJpn,1987;38:5673VestGE.MetalFinishing,1967;65:824郭忠诚.有色金属(季刊),1994:46:675郭忠诚,材料保护,1991:24:15
[1] WANG Jingyang, SUN Luchao, LUO Yixiu, TIAN Zhilin, REN Xiaomin, ZHANG Jie. Rare Earth Silicate Environmental Barrier Coating Material: High-Entropy Design and Resistance to CMAS Corrosion[J]. 金属学报, 2023, 59(4): 523-536.
[2] YANG Tianye, CUI Li, HE Dingyong, HUANG Hui. Enhancement of Microstructure and Mechanical Property of AlSi10Mg-Er-Zr Alloys Fabricated by Selective Laser Melting[J]. 金属学报, 2022, 58(9): 1108-1117.
[3] LI Min, LI Haoze, WANG Jijie, MA Yingche, LIU Kui. Effect of Ce on the Microstructure, High-Temperature Tensile Properties, and Fracture Mode of Strip Casting Non-Oriented 6.5%Si Electrical Steel[J]. 金属学报, 2022, 58(5): 637-648.
[4] LIU Jie, XU Le, SHI Chao, YANG Shaopeng, HE Xiaofei, WANG Maoqiu, SHI Jie. Effect of Rare Earth Ce on Sulfide Characteristics and Microstructure in Non-Quenched and Tempered Steel[J]. 金属学报, 2022, 58(3): 365-374.
[5] LIU Zhongwu, HE Jiayi. Several Issues on the Development of Grain Boundary Diffusion Process for Nd-Fe-B Permanent Magnets[J]. 金属学报, 2021, 57(9): 1155-1170.
[6] LU Bin, CHEN Furong, ZHI Jianguo, GENG Ruming. Enhanced Welding Properties of High Strength Steel via Rare Earth Oxide Metallurgy Technology[J]. 金属学报, 2020, 56(9): 1206-1216.
[7] ZHU Jian, ZHANG Zhihao, XIE Jianxin. Plastic Deformation Behavior and Fracture Mechanism of Rare Earth H13 Steel Based on In Situ TEM Tensile Study[J]. 金属学报, 2020, 56(12): 1592-1604.
[8] HUANG Yu, CHENG Guoguang, LI Shijian, DAI Weixing. Precipitation Mechanism and Thermal Stability of Primary Carbide in Ce Microalloyed H13 Steel[J]. 金属学报, 2019, 55(12): 1487-1494.
[9] Yu HUANG, Guoguang CHENG, You XIE. Modification Mechanism of Cerium on the Inclusions in Drill Steel[J]. 金属学报, 2018, 54(9): 1253-1261.
[10] Xuan YU, Zhihao ZHANG, Jianxin XIE. Microstructure, Ordered Structure and Warm TensileDuctility of Fe-6.5%Si Alloy with Various Ce Content[J]. 金属学报, 2017, 53(8): 927-936.
[11] Xiaowei ZHOU,Chun OUYANG,Yanxin QIAO,Yifu SHEN. Analysis of Toughness and Strengthening Mechanisms forNi-CeO2 Nanocomposites Coated on the ActivatedSurface of Ti Substrate[J]. 金属学报, 2017, 53(2): 140-152.
[12] LIU Zheng, LIU Xiaomei, ZHU Tao, CHEN Qingchun. EFFECTS OF ELECTROMAGNETIC STIRRING WITH LOW CURRENT FREQUENCY ON RE DISTRIBUTION IN SEMISOLID ALUMINUM ALLOY[J]. 金属学报, 2015, 51(3): 272-280.
[13] YAO Zhanquan, ZHAO Zengqi, JIANG Liping,HAO Hongbo, WU Shuangxia,ZHANG Guangrui, YANG Jiandong. EFFECTS OF Ce ADDITION ON THE MICROSTRUCTURE AND MAGNETOSTRICTION OF Fe83Ga17 ALLOY[J]. 金属学报, 2013, 49(1): 87-91.
[14] ZHANG Hui WANG Shaoqing. FIRST-PRINCIPLES STUDY ON THE PHASE STABILITY OF Mg-La AND Mg-Nd BINARY ALLOYS[J]. 金属学报, 2012, 48(7): 889-894.
[15] XU Liang TANG Junlei ZUO Yu. ELECTROPLATING OF Cr-Pd ALLOY ON 316L STAINLESS STEEL AND ITS CORROSION RESISFANCE IN THE STRONG REDUCING MEDIUMS[J]. 金属学报, 2011, 47(2): 209-213.
No Suggested Reading articles found!