| SOLIDIFICATION THEORY AND RAPID SOLIDIFICATION |
| SHEN Ningfu; TANG Yali; GUAN Shaokang; ZHANG Dongjie (Zhengzhou Institute of Technology; Zhengzhou 450002)(Manuscript received 1995-12-28) |
|
Cite this article:
SHEN Ningfu; TANG Yali; GUAN Shaokang; ZHANG Dongjie (Zhengzhou Institute of Technology; Zhengzhou 450002)(Manuscript received 1995-12-28). SOLIDIFICATION THEORY AND RAPID SOLIDIFICATION. Acta Metall Sin, 1996, 32(7): 673-684.
|
|
|
Abstract Recent progress in solidification theory related to the high growth rate during rapid solidification has been summarized. Methods for quantitative analyses of non-equilibrium partition coefficient, nucleation incubation time, phase selection, absolute stability of planar interface, rapid dendrite or cell growth as well as solidification development in a bulk specimen have been presented.Correspondent: SHEN Ningfu, professor,Research Centre for Materials, Zhengzhou Institute of Technology,Zhengzhou 450002
|
|
Received: 18 July 1996
|
| 1KurzW,FisherDJ.FundamentalsofSolidification,Thirdedition,Switzerland:TransTech,1989:1372 AzizMJ.JApplPhys,1982;53:11583沈宁福.铸造,1990;2:214 KeltonKF,GreerAL.JNon-CrystSolids,1986;79:2955ShaoGS,TsakiropoulosP.ActaMetallMater.1994;42:29376AdkinsNJE,SaundersN,TsakiropoulosP.MaterSciEng,1988;98:2177邵国胜,沈宁福.材料科学进展,1992;6:3938TangYL,ShenNF.JAlloysCompounds,1993;201:L219关绍康,汤亚力,沈宁福,胡汉起.金属学报,1994;30:A15010BoettingerWJ,PerepezkoJH.RapidlySolidifiedCrystallineAlloys,AIME,1985:2111LeviCG.MetallTrans,1988;19A:68712MullinsWW,SekerkaRF.JApplPhys,1964;35:44413SekerkaRF.JCrystalGrowth,1968;3:7114TrivediR,KurzW.ActaMetall,1986;34:166315TrivediR,LiptonJ,KurzW.ActaMetall,1987;35:96516LiptonJ,KurzW,TrivediR.ActaMetall,1987;35:95717LiptonJ,GlicksmanME,KurzW.MaterSciEng,1984;65:5718KurzW,TrivediR.ActaMetallMater,1990;38:119BoettingerWJ,BenderskyL,EarlyJG.MetallTrans,1986;17A:78120ShaoGS,TsakiropoulosP,MiodownikAP.IntJRapidSolidification,1993;8:4121JonesH.MaterSciEng,1991;A133:3322沈宁福,汤亚力,关绍康,张东捷.'94秋季中国材料科学研讨 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|