OXIDATION MECHANISM OF BINARY Ti-Al ALLOYS AT ELEVATED TEMPERATURE
LI Xiangyang;ZHANG Yonggang;CHEN Changqi(Beijing University of Aeronautics andAstronautics; Beijing 100083); ZHANG Xiaoji;ZHANG Tonghe;ZHANG Huixing (Beijing Normal University; Beiing 100875)
Cite this article: 

LI Xiangyang;ZHANG Yonggang;CHEN Changqi(Beijing University of Aeronautics andAstronautics; Beijing 100083); ZHANG Xiaoji;ZHANG Tonghe;ZHANG Huixing (Beijing Normal University; Beiing 100875). OXIDATION MECHANISM OF BINARY Ti-Al ALLOYS AT ELEVATED TEMPERATURE. Acta Metall Sin, 1997, 33(9): 964-970.

Download:  PDF(2077KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The isothermal oxidation behavior of Ti-33.3% Al, Ti-48% Al and Ti-52%Al(atomic fraction) intermetallic compounds oxidated at 1073 and 1173K in air was investigated. The reaction products of the oxidation scale were examined by XRD, and the surface morphology and cross-section microstructure of the oxidation scale were analyzed by SEM equipped with EDS. The results indicated that the oxidation scale of binary Ti-Al alloys was consisted of a series of thin layers, and the oxidation process could be classified into three steps, the growing direction of the oxidation scale and the rate-controlling factor of various steps is somewhat different; the isothermal oxidation kinetic curves mainly follow parabolic rate law.
Key words:  Ti-Al intermetallic compound      high temperature oxidation      oxidation scale      oxidation kinetics     
Received:  18 September 1997     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1997/V33/I9/964

1Kim Y W JOM,1989;41(7):24
2Kim Y W,Dimidak D M.JOM,1991;43(8):40
3Shida Y,Anada H Corros Sci,1993;35:943
4Taniguchi S,Shibata T,Itoh S.Mater Trans Jpn Inst Met,1991;32:151
[1] XU Wenguo, HAO Wenjiang, LI Yingju, ZHAO Qingbin, LU Bingyu, GUO Heyi, LIU Tianyu, FENG Xiaohui, YANG Yuansheng. Effects of Trace Aluminum and Titanium on High Temper-ature Oxidation Behavior of Inconel 690 Alloy[J]. 金属学报, 2023, 59(12): 1547-1558.
[2] XIE Leipeng, SUN Wenyao, CHEN Minghui, WANG Jinlong, WANG Fuhui. Effects of Processing on Microstructures and Properties of FGH4097 Superalloy[J]. 金属学报, 2022, 58(8): 992-1002.
[3] YANG Liang, LV Haotian, WAN Chunlei, GONG Qianming, CHEN Hao, ZHANG Chi, YANG Zhigang. Review: Mechanism of Reactive Element Effect—Oxide Pegging[J]. 金属学报, 2021, 57(2): 182-190.
[4] Mingyu ZHAO,Huijuan ZHEN,Zhihong DONG,Xiuying YANG,Xiao PENG. Preparation and Performance of a Novel Wear-Resistant and High Temperature Oxidation-Resistant NiCrAlSiC Composite Coating[J]. 金属学报, 2019, 55(7): 902-910.
[5] GAO Bo, WANG Lei, SONG Xiu, LIU Yang, YANG Shuyu, CHIBA Akihiko. Effect of Pre-Oxidation on High Temperature Oxidation and Corrosion Behavior of Co-Al-W-Based Superalloy[J]. 金属学报, 2019, 55(10): 1273-1281.
[6] Yin BAI, Zhengdong LIU, Jianxin XIE, Hansheng BAO, Zhengzong CHEN. Effect of Pre-Oxidation Treatment on the Behavior of High Temperature Oxidation in Steam of G115 Steel[J]. 金属学报, 2018, 54(6): 895-904.
[7] Wenying ZHANG, Jun LI, Bo ZHOU. OXIDATION KINETICS BEHAVIOR AND ELECTRICAL PROPERTY OF MnCO2O4 SPINEL AS A COATING MATERIAL FOR METALLIC INTERCONNECTS[J]. 金属学报, 2016, 52(3): 355-360.
[8] Yuxiang ZENG,Xiping GUO,Yanqiang QIAO,Zhongyi NIE. EFFECT OF Zr ADDITION ON MICROSTRUCTURE AND OXIDATION RESISTANCE OF Nb-Ti-Si BASE ULTRAHIGH-TEMPERATURE ALLOYS[J]. 金属学报, 2015, 51(9): 1049-1058.
[9] Haigen ZHAO,Shusuo LI,Yanling PEI,Shengkai GONG,Huibin XU. MICROSTRUCTURE AND MECHANICAL PROPERTIES OF Ni3Al-BASED SINGLE CRYSTSAL ALLOY IC21[J]. 金属学报, 2015, 51(10): 1279-1287.
[10] ZHOU Xiaowei SHEN Yifu GU Dongdong. MICROSTRUCTURE AND HIGH TEMPERATURE OXIDATION RESISTANCE OF NANOCRYSTALLINE Ni–CeO2 COMPOSITE COATINGS DEPOSITED BY DOUBLE–PULSED ELECTRO DEPOSITION[J]. 金属学报, 2012, 48(8): 957-964.
[11] YU Daqian, LU Xuyang, MA Jun, JIANG Sumeng, LIU Shanchuan, GONG Jun, SUN Chao. STUDY OF OXIDATION BEHAVIOR OF THE GRADIENT NiCrAlY COATING AT 1000 AND 1100 ℃[J]. 金属学报, 2012, 48(6): 759-768.
[12] QIU Jun ZHAO Wenjin Thomas Guilbert Jean-Luc Bechade. HIGH TEMPERATURE OXIDATION BEHAVIOURS OF THREE ZIRCONIUM ALLOYS[J]. 金属学报, 2011, 47(9): 1216-1220.
[13] SONG Peng LU Jiansheng ZHANG Defeng LU Jianguo LI Dejiang. EFFECT OF La AND Hf DOPANT ON THE HIGH TEMPERATURE OXIDATION OF CoNiCrAl ALLOYS[J]. 金属学报, 2011, 47(6): 655-662.
[14] PENG Xin JIANG Sumeng DUAN Xuhai GONG Jun SUN Chao. HIGH TEMPERATURE OXIDATION BEHAVIOR OF A (MCrAlY+AlSiY) COMPOSITE COATING[J]. 金属学报, 2009, 45(3): 378-384.
[15] . [J]. 金属学报, 2007, 43(6): 625-630 .
No Suggested Reading articles found!