| OXIDATION MECHANISM OF BINARY Ti-Al ALLOYS AT ELEVATED TEMPERATURE |
| LI Xiangyang;ZHANG Yonggang;CHEN Changqi(Beijing University of Aeronautics andAstronautics; Beijing 100083); ZHANG Xiaoji;ZHANG Tonghe;ZHANG Huixing (Beijing Normal University; Beiing 100875) |
|
Cite this article:
LI Xiangyang;ZHANG Yonggang;CHEN Changqi(Beijing University of Aeronautics andAstronautics; Beijing 100083); ZHANG Xiaoji;ZHANG Tonghe;ZHANG Huixing (Beijing Normal University; Beiing 100875). OXIDATION MECHANISM OF BINARY Ti-Al ALLOYS AT ELEVATED TEMPERATURE. Acta Metall Sin, 1997, 33(9): 964-970.
|
|
|
Abstract The isothermal oxidation behavior of Ti-33.3% Al, Ti-48% Al and Ti-52%Al(atomic fraction) intermetallic compounds oxidated at 1073 and 1173K in air was investigated. The reaction products of the oxidation scale were examined by XRD, and the surface morphology and cross-section microstructure of the oxidation scale were analyzed by SEM equipped with EDS. The results indicated that the oxidation scale of binary Ti-Al alloys was consisted of a series of thin layers, and the oxidation process could be classified into three steps, the growing direction of the oxidation scale and the rate-controlling factor of various steps is somewhat different; the isothermal oxidation kinetic curves mainly follow parabolic rate law.
|
|
Received: 18 September 1997
|
1Kim Y W JOM,1989;41(7):24 2Kim Y W,Dimidak D M.JOM,1991;43(8):40 3Shida Y,Anada H Corros Sci,1993;35:943 4Taniguchi S,Shibata T,Itoh S.Mater Trans Jpn Inst Met,1991;32:151 |