| POSITRON ANNIHILATION STUDY ON THE EFFECT OF MISCH METAL IN Al-Fe-V-Si-Mm ALLOYS |
| JIA Wei;XIONG Lianggue;ZENG Meiguang;WANG Jiangiang (Department of Materials Science; College of Science; Northeastern University; Shenyang 110006)(International Center for Materials Physics; Institute of Matal Research; The Chinese Academy of Sciences;Shenyang 110015) |
|
Cite this article:
JIA Wei;XIONG Lianggue;ZENG Meiguang;WANG Jiangiang (Department of Materials Science; College of Science; Northeastern University; Shenyang 110006)(International Center for Materials Physics; Institute of Matal Research; The Chinese Academy of Sciences;Shenyang 110015). POSITRON ANNIHILATION STUDY ON THE EFFECT OF MISCH METAL IN Al-Fe-V-Si-Mm ALLOYS. Acta Metall Sin, 1998, 34(2): 221-224.
|
|
|
Abstract The positron lifetime spectra of several Al-Fe-V-Si-Mm alloys with different content of Misch metal was measured, and the effect of the amount of Misch metal on the positron lifetime in Al-Fe-V-Si-Mm alloys was discussed.
|
|
Received: 18 February 1998
|
1Davis L A, Das S K, Li J C M, Zedalis M S. Inter,J Rapid Solidifi, 1994; 8: 110 2 Das S K and Froes F H. In: Liebermain H H ed., Rapidly Solidified Alloys, Marcel Dekker Inc, 1993: 339 3曾梅光,王建强,钱存富,张宝金,陈秀芳94秋季中国材料讨论会文集,1994;12:660(Zeng M G,Wang J Q,Qian C F,Zhang B J,Chen X F. ’94 C-MRS Materials Conference Proceedings.1994;12:660) 4 Kirgarrd P, Eldtup M, Mogensen O E, Peterson N. Comput Phys Commun,1981; 23: 307 5 Sui M L, Xiong L Y, Deng W, Lu K, Pain S, He Y Z.J Appl Phys, 1991;69: 4451 6 Sui M L, Lu K, Deng W, Xiong L. Y, Patu S, He Y Z. Phys Rev 1991; 44B: 6466 7Liu X D,Wang J T,Zhu J.J Mater Sci,1994;29:929 8 Wang J Q, Chao Y S, Zeng M G, Zhang B J, Chen X F.J Rare Earth, 1996; 14: 201 9Lu K.Mater,Sci Eng,1996;R16:161 10 MacKenziet I K. In: Brandt W, Dupasquier A eds, Positron Solid-state Physics, North-Holland Publishing CO, 1983: 200 11 Schaefer H E,Wurschum R,Birringer R,Gleiter H. Phys Rev,1988;38:9545T |