Please wait a minute...
Acta Metall Sin  1998, Vol. 34 Issue (5): 459-466    DOI:
Current Issue | Archive | Adv Search |
THE NEW DEVELOPMENT OF THE SELF-SReM4 MODEL AND ITS APPLICATION TO THE QUARTERNARY SYSTEM OF C-Mn-Fe-Si
XU Kuangdi;JIANG Guochang; ZHANG Xiaobing; TANG Kai; XU Jianlun; DING Weizhong (Shanghai Enhaned Laboratory of Ferrometallurgy; Shanghai University; Shanghai 200072)
Cite this article: 

XU Kuangdi;JIANG Guochang; ZHANG Xiaobing; TANG Kai; XU Jianlun; DING Weizhong (Shanghai Enhaned Laboratory of Ferrometallurgy; Shanghai University; Shanghai 200072). THE NEW DEVELOPMENT OF THE SELF-SReM4 MODEL AND ITS APPLICATION TO THE QUARTERNARY SYSTEM OF C-Mn-Fe-Si. Acta Metall Sin, 1998, 34(5): 459-466.

Download:  PDF(555KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  On the base of sub-regular melt model (SELF-SReM4.0 model), a model SELF-SReM4.1 was designed to solve the precipitate of carbide. Taking C-Mn-Fe-Si quarternary system as an example, the calculated results of component activities by above mentioned two models are introduced and some equilibrium rules of Si-Mn and Mn-Fe systems are also analysed.
Key words:  C-Mn-Fe-Si quarternary system      thermodynamics      sub-regular melt model     
Received:  18 May 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I5/459

1Zhang X B, Jiang G C, Tang K, Xu J J, Ding W Z, Xu K D. Calphad, 1997; 21(3)
2Katsnelson A, Tsukihashi F, Sano N ISIJ Int, 1993, 33: 1045
3Hultgren R.Selected Values of Therrnodynamic Properties of Metals and Alloys,1973:487
4Tanaka A. Trans Jpn Inst Met, 1979; 20: 516
5Gee R, Rosenqvist T Scand J Met, 1978; 7: 38
6Ding W Z.PhD Dissertation,Trondheim Unversity,Norway,1993
7Chipman J, Alfred R M, Gott L W, Small R B, Wilsong M D, Thomson C N; Guernsey D L, Fulton C J.Trans AIME, 1952 44:1215
8Darken L S. Trans Met Soc AIME, 1967 239: 90
9Schrmann E,Kramer Giessereiforschung,1969;21:29
10Tuset J Kr, Sandvik J. SINTEF Res Rep 340558, 1970
11Kubaschewski O, Alcock C B. Metall Thermochem. 5th ed, Oxford: Pengramon Press, 1979: 376
12周国冶.金属学报,19972 33:126(Zhou Guozhi.Acta Metall Sin,1997;33:126)
13丁学勇,范鹏,韩其勇.金属学报,1994;30:B49(Ding Xueyong,Fan Peng;Han Qiyong Acta Metall Sin,1994; 30:B49)"
[1] ZHANG Yuexin, WANG Jujin, YANG Wen, ZHANG Lifeng. Effect of Cooling Rate on the Evolution of Nonmetallic Inclusions in a Pipeline Steel[J]. 金属学报, 2023, 59(12): 1603-1612.
[2] GAO Jianbao, LI Zhicheng, LIU Jia, ZHANG Jinliang, SONG Bo, ZHANG Lijun. Current Situation and Prospect of Computationally Assisted Design in High-Performance Additive Manufactured Aluminum Alloys: A Review[J]. 金属学报, 2023, 59(1): 87-105.
[3] LIU Feng, WANG Tianle. Precipitation Modeling via the Synergy of Thermodynamics and Kinetics[J]. 金属学报, 2021, 57(1): 55-70.
[4] WANG Zumin,ZHANG An,CHEN Yuanyuan,HUANG Yuan,WANG Jiangyong. Research Progress on Fundamentals and Applications of Metal-Induced Crystallization[J]. 金属学报, 2020, 56(1): 66-82.
[5] Chengming ZHENG, Qingchao TIAN. Effect of Alloy Elements on Oxidation Behavior of Piercing Plug Steel[J]. 金属学报, 2019, 55(4): 427-435.
[6] Liheng LIU,Chunshan CHE,Gang KONG,Jintang LU,Shuanghong ZHANG. DESTABILIZATION MECHANISM OF Fe-Al INHIBITION LAYER IN Zn-0.2%Al HOT-DIP GALVANIZING COATING AND RELATED THERMODYNAMIC EVALUATION[J]. 金属学报, 2016, 52(5): 614-624.
[7] Feng LIU, Kang WANG. DISCUSSIONS ON THE CORRELATION BETWEEN THERMODYNAMICS AND KINETICS DURING THE PHASE TRANSFORMATIONS IN THE TMCP OF LOW-ALLOY STEELS[J]. 金属学报, 2016, 52(10): 1326-1332.
[8] XIE Jun, YU Jinjiang, SUN Xiaofeng, JIN Tao, SUN Yuan. CARBIDE EVOLUTION BEHAVIOR OF K416B AS-CAST Ni-BASED SUPERALLOY WITH HIGH W CONTENT DURING HIGH TEMPERATURE CREEP[J]. 金属学报, 2015, 51(4): 458-464.
[9] WU Changjun, ZHU Chenlu, SU Xuping, LIU Ya, PENG Haoping, WANG Jianhua. THERMODYNAMICAL AND KINETIC INVESTIGA-TION OF FORMATION OF PERIODIC LAYERED STRUCTURE IN TiCu/Zn INTERFACE REACTION[J]. 金属学报, 2014, 50(8): 930-936.
[10] MA Ping, WU Erdong, LI Wuhui, SUN Kai, CHEN Dongfeng. MICROSTRUCTURES AND HYDROGEN STORAGE PROPERTIES OF Ti0.7Zr0.3(Cr1-xVx)2 ALLOYS[J]. 金属学报, 2014, 50(4): 454-462.
[11] WANG Bin, LIU Zhenyu, ZHOU Xiaoguang, WANG Guodong. CALCULATION OF TRANSFORMATION DRIVING FORCE FOR THE PRECIPITATION OF NANO-SCALED CEMENTITES IN THE HYPOEUTECTOID STEELS THROUGH ULTRA FAST COOLING[J]. 金属学报, 2013, 49(1): 26-34.
[12] LI Wuhui TIAN Baohong MA Ping WU Erdong. HYDROGEN STORAGE PROPERTIES OF ScMn2 ALLOY[J]. 金属学报, 2012, 48(7): 822-829.
[13] WU Chaofeng MA Mingxing WU Aiping LIU Wenjin ZHONG Minlin ZHANG Weiming ZHANG Hongjun. MORPHOLOGIC CHARACTERISTICS OF IN SITU SYNTHESIZED CARBIDE PARTICLES IN LASER CLADDED Fe-BASED COMPOSITE COATINGS[J]. 金属学报, 2009, 45(9): 1091-1098.
[14] PENG Ningqi TANG Guangbo LIU Zhengdong WU Xiuyue. MODIFICATION OF ZENER'S TWO--PARAMETER IN THE SUPERELEMENT MODEL FOR Fe--Σ Xi--C ALLOY SYSTEMS[J]. 金属学报, 2009, 45(3): 331-337.
[15] MA Yingche WANG Weidong CHEN Bo GAO Ming LIU Kui LI Yiyi. INTERFACE REACTION BETWEEN CERAMIC MOULDS AND Ti46Al1B AS--CAST VALVES[J]. 金属学报, 2009, 45(3): 369-373.
No Suggested Reading articles found!