LASER SURFACE ALLOYING OF TiAl INTERMETALLICS WITH CARBON
HE Xiuli; WANG Huaming (Department of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083)ZHENG Qiguang; XU Desheng (State Key Laboratory of Laser Technology; Huazhong University of Science and Technology; Wuhan 430074)Correspondent: WANG Huaming; professor Tel: (010)62017251-7034(O); (010)62013322-5294(H);Fax: (010)62015920; E-mail: Wanghm@mailcity.com
Cite this article: 

HE Xiuli; WANG Huaming (Department of Materials Science and Engineering; Beijing University of Aeronautics and Astronautics; Beijing 100083)ZHENG Qiguang; XU Desheng (State Key Laboratory of Laser Technology; Huazhong University of Science and Technology; Wuhan 430074)Correspondent: WANG Huaming; professor Tel: (010)62017251-7034(O); (010)62013322-5294(H);Fax: (010)62015920; E-mail: Wanghm@mailcity.com. LASER SURFACE ALLOYING OF TiAl INTERMETALLICS WITH CARBON. Acta Metall Sin, 1998, 34(9): 983-986.

Download:  PDF(1616KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Laser surface alloying with carbon was employed to modify the surface properties of TiAl intermetallics. The rapidly solidified "in-situ" wear resistant composite reinforced by titanium carbide was produced in the laser modified surface layer. The microstructure of the laser alloyed surface layer was studied as a function of the laser processing parameters.
Key words:  TiAl intermetallics      TiC      laser surface alloying     
Received:  18 September 1998     
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y1998/V34/I9/983

1Kim Y W.JOM,1989; 41(7):24
2 Lipsitt H A, Shechtman D, Schafrik R E. Metall Trans, 1975; 6A: 1975
3 Xu D, Zheng Z, Liu X, Zou S, TaniguchiS, Shibata T, Yamada T. Surf Coat Technol,1994; 66: 486
4Kim Y W. Acta Metall Mater, 1992;40:1121
5 Noda T, Okabe M, Isobe G. Mater Sci Eng; 1996; A213: 157
6王华明.金属学报,1997;33:917(Wang H M. Acta Metall Sin, 1997 33: 917)
[1] ZHENG Liang, ZHANG Qiang, LI Zhou, ZHANG Guoqing. Effects of Oxygen Increasing/Decreasing Processes on Surface Characteristics of Superalloy Powders and Properties of Their Bulk Alloy Counterparts: Powders Storage and Degassing[J]. 金属学报, 2023, 59(9): 1265-1278.
[2] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
[3] LIU Xingjun, WEI Zhenbang, LU Yong, HAN Jiajia, SHI Rongpei, WANG Cuiping. Progress on the Diffusion Kinetics of Novel Co-based and Nb-Si-based Superalloys[J]. 金属学报, 2023, 59(8): 969-985.
[4] XU Yongsheng, ZHANG Weigang, XU Lingchao, DAN Wenjiao. Simulation of Deformation Coordination and Hardening Behavior in Ferrite-Ferrite Grain Boundary[J]. 金属学报, 2023, 59(8): 1042-1050.
[5] ZHANG Lu, YU Zhiwei, ZHANG Leicheng, JIANG Rong, SONG Yingdong. Thermo-Mechanical Fatigue Cycle Damage Mechanism and Numerical Simulation of GH4169 Superalloy[J]. 金属学报, 2023, 59(7): 871-883.
[6] LU Yuhua, WANG Haizhou, LI Dongling, FU Rui, LI Fulin, SHI Hui. A Quantitative and Statistical Method of γ' Precipitates in Superalloy Based on the High-Throughput Field Emission Scanning Eelectron Microscope[J]. 金属学报, 2023, 59(7): 841-854.
[7] ZHANG Qiliang, WANG Yuchao, LI Guangda, LI Xianjun, HUANG Yi, XU Yunze. Erosion-Corrosion Performance of EH36 Steel Under Sand Impacts of Different Particle Sizes[J]. 金属学报, 2023, 59(7): 893-904.
[8] ZHAO Pingping, SONG Yingwei, DONG Kaihui, HAN En-Hou. Synergistic Effect Mechanism of Different Ions on the Electrochemical Corrosion Behavior of TC4 Titanium Alloy[J]. 金属学报, 2023, 59(7): 939-946.
[9] ZHANG Deyin, HAO Xu, JIA Baorui, WU Haoyang, QIN Mingli, QU Xuanhui. Effects of Y2O3 Content on Properties of Fe-Y2O3 Nanocomposite Powders Synthesized by a Combustion-Based Route[J]. 金属学报, 2023, 59(6): 757-766.
[10] LI Qian, LIU Kai, ZHAO Tianliang. Rust Formation Behavior and Mechanism of Q235 Carbon Steel in 5%NaCl Salt Spray Under Elastic Tensile Stress[J]. 金属学报, 2023, 59(6): 829-840.
[11] XU Lei, TIAN Xiaosheng, WU Jie, LU Zhengguan, YANG Rui. Microstructure and Mechanical Properties of Inconel 718 Powder Alloy Prepared by Hot Isostatic Pressing[J]. 金属学报, 2023, 59(5): 693-702.
[12] WANG Changsheng, FU Huadong, ZHANG Hongtao, XIE Jianxin. Effect of Cold-Rolling Deformation on Microstructure, Properties, and Precipitation Behavior of High-Performance Cu-Ni-Si Alloys[J]. 金属学报, 2023, 59(5): 585-598.
[13] LIU Jihao, ZHOU Jian, WU Huibin, MA Dangshen, XU Huixia, MA Zhijun. Segregation and Solidification Mechanism in Spray-Formed M3 High-Speed Steel[J]. 金属学报, 2023, 59(5): 599-610.
[14] WU Xinqiang, RONG Lijian, TAN Jibo, CHEN Shenghu, HU Xiaofeng, ZHANG Yangpeng, ZHANG Ziyu. Research Advance on Liquid Lead-Bismuth Eutectic Corrosion Resistant Si Enhanced Ferritic/Martensitic and Austenitic Stainless Steels[J]. 金属学报, 2023, 59(4): 502-512.
[15] MA Zongyi, XIAO Bolv, ZHANG Junfan, ZHU Shize, WANG Dong. Overview of Research and Development for Aluminum Matrix Composites Driven by Aerospace Equipment Demand[J]. 金属学报, 2023, 59(4): 457-466.
No Suggested Reading articles found!