| [1] Gao K, Wang L D, Zhu M, Cheng J D, Shi Y J, Kang M K. Acta Metall Sin, 2007; 43: 315
(高宽, 王六定, 朱明, 陈景东, 施易军, 康沫狂. 金属学报, 2007; 43: 315)
[2] Yang H S, Bhadeshia H K D H. Mater Sci Technol, 2008; 25: 335
[3] Caballero F G, Bhadeshia H K D H, Mawella K J A, Jones D G, Brown P. Mater Sci Technol, 2001; 17: 517
[4] Keehan E, Karlsson L, Andren H O, Bhadeshia H K D H. Sci Technol Weld Joining, 2006; 11: 10
[5] Caballero F G, Bhadeshia H K D H. Curr Opin Solid State Mater Sci, 2004; 8: 251
[6] Zhang M X. PhD Thesis, Northwestern Polytechnical Univesity, 1990
(张明星. 博士学位论文, 西北工业大学, 1990)
[7] Keehan E, Karlsson L, Andren H O, Bhadeshia H K D H. Sci Technol Weld Joining, 2006; 11: 1
[8] Kang M K, Sun J L, Yang Q M. Metall Trans, 1990; 21A: 853
[9] Wang L D, Zhu M, Zhou W M, Chen J D, Shi Y J, Chen G D, Zhang Q. Mater Sci Forum, 2007; 539–543: 4562
[10] Wang L D, Zhu M, Chen J D, Shi Y J, Chen G D. Trans Mater Heat Treat, 2007; 28: 43
(王六定, 朱明, 陈景东, 施易军, 陈国栋. 材料热处理学报, 2007; 28: 43)
[11] Guo Z. PhD Thesis, University of California, Berkeley, USA, 2001
[12] Zhao W Y, Wang Q Y, Sun Z Y, Ye X X. J Chin Electron Microsc Soc, 1999; 18: 549
(赵文俞, 王勤燕, 孙振亚, 叶先贤. 电子显微学报, 1999; 18: 549)
[13] Zhang M X, Wang J, Kang M K. Phys Test Chem Anal (Phys Test), 1993; 29(2): 6
(张明星, 王军, 康沫狂. 理化检验(物理分册), 1993; 29(2): 6)
[14] Kozeschnik E, Bhadeshia H K D H. Mater Sci Technol, 2008; 24: 343
[15] Wang X T. Metal Materials. Beijing: China Machine Press, 1987: 1
(王笑天. 金属材料学. 北京: 机械工业出版社, 1987: 1)
[16] Hossein N S, Movaghar G M R, Nili A M, Shirazi H. Mater Sci Eng, 2008; A473: 251
[17] Peet M, Babu S S, Miller M K, Bhadeshia H K D H. Scr Mater, 2004; 50: 1279
[18] Caballero F G, Miller M K, Babu S S, Garcia–Mateo C. Acta Mater, 2007; 55: 386
[19] Caballero F G, Miller M K, Garcia–Mateo C, Capdevila C, Babu S S. Acta Mater, 2007; 56: 191
[20] Jacques P J. Curr Opin Solid State Mater Sci, 2004; 8: 260
[21] Bhadeshia H K D H. Bainite in Steels. 2nd Ed., London: Institute of Materials, 2001: 28
[22] Smith G M. PhD Thesis, University of Cambridge, 1984
[23] Singh S B, Bhadeshia H K D H. Mater Sci Eng, 1998; A245: 72
[24] Bhadeshia H K D H. Mater Sci Eng, 2008; A481–482: 36
[25] Hu G L, Xie XW. Heat Treatment of Steel. 2nd Ed., Xi’an: Northwestern Polytechnical University Press, 2008: 298
(胡光立, 谢希文. 钢的热处理. 第2版, 西安: 西北工业大学出版社, 2008: 298) |