| OPTIMIZED COMPOSITIONS OF Ti-(Cu, Ni)-Sn ALLOY FOR METALLIC GLASS FORMATION AND THEIR CORRELATION WITH EUTECTIC REACTION |
| LIU Yuanshuai; XU Jian |
| Shenyang National Laboratory for Materials Science; Institute of Metal Research; Chinese Academy of Sciences |
|
Cite this article:
LIU Yuanshuai XU Jian. OPTIMIZED COMPOSITIONS OF Ti-(Cu, Ni)-Sn ALLOY FOR METALLIC GLASS FORMATION AND THEIR CORRELATION WITH EUTECTIC REACTION. Acta Metall Sin, 2008, 44(12): 1424-1430.
|
|
|
Abstract Adopting the “3D pinpointing approach”, compositional dependence of glass--forming ability (GFA) for Ti-(Cu1-xNix)-Sn (0.20≤x≤0.30, atomic fraction) quaternary alloys was systematically investigated. The alloy with the optimized GFA is located at Ti38Cu37.8Ni16.2Sn8. Its critical diameter for metallic glass formation is near 1.0 mm for the rods fabricated using Cu mold casting. This metallic glass exhibits the supercooled liquid region ΔTx of 56 K and the reduced glass transition temperature Trg of 0.57. By characterizing the microstructure of the arc-melted Ti38Cu37.8Ni16.2Sn8 alloy, it is indicated that solidification of the alloy melt undergoes a pseudo-binary eutectic reaction of L→Ti5Sn3Cu+TiCuNi.
|
|
Received: 26 March 2008
|
|
|
[1]Johnson W L.MRS Bull,1999;24:42 [2]Inoue A.Acta Mater,2000;28:279 [3]Greet A L,Ma E.MRS Bull,2007;32:611 [4]Li Y,Poon S J,Shiflet G J,Xu J,Kim D H,L(?)ffler J F. MRS Bull,2007;32:624 [5]Kim Y C,Kim W T,Kim D H.Mater Sci Eng,2004; A375-377:127 [6]Men H,Pang S,Inoue A,Zhang T.Mater Trans,2005; 46:2218 [7]Kim K B,Das J,Wang X D,Zhang X,Eckert J,Yi S. Philos Mag Lett,2006;86:479 [8]Ohkubo T,Nagahama D,Mukai T,Hono K.J Mater Res, 2007;22:1406 [9]Qin F X,Wang X M,Kawashima A,Zhu S L,Kimura H, Inoue A.Mater Trans,2006;47:1934 [10]Guo F Q,Wang H J,Poon S J,Shiflet G J.Appl Phys Lett,2005;86:091907 [11]Duan G,Wiest A,Lind M L,Kahl A,Johnson W L.Scr Mater,2008:58:465 [12]Zhang Q S,Zhang W,Inoue A.Mater Trans,2007;48: 3031 [13]Jiang Q K,Wang X D,Nie X P,Zhang G Q,Ma H,Feeht H J,Bendnarcik J,Franz H,Lin Y G,Cao Q P,Jiang J Z.Acta Mater,2008;56:1785 [14]Dai C L,Guo H,Shen Y,Li Y,Ma E,Xu J.Scr Mater, 2006;54:1403 [15]Shen Y,Ma E,Xu J.d Mater Sci Technol,2008;24:149 [16]Ma H,Shi L L,Xu J,Li Y,Ma E.Appl Phys Lett,20051 87:181915 [17]Zheng Q,Xu J,Ma E.J Appl Phys,2007;102:113519 [18]Lu Z P,Liu C T,Thompson J R,Porter W D.Phys Rev Lett,2004;92:245503 [19]Ponnambalam V,Poon S J,Shiflet G J.J Mater Res,2004; 19:1320 [20]Shen J,Chen Q J,Sun F J,Fan H B,Wang G.Appl Phys Lett,2005;86:151907 [21]Zhang T,Inoue A.Mater Trans JIM,1998;39:1001 [22]Zhang T,Inoue A.Mater Sci Eng,2001;A304-306:771 [23]Ma C L,Ishihara S,Soejima H,Nishiyama N,Inoue A. Mater Trans,2004;45:1802 [24]Huang Y J,Shen J,Sun J F,Yu X B.J Alloys Compd, 2007;427:171 [25]Wang Y L,Ma E,Xu J.Philos Mag Lett,2008;88:319 [26]Ma H,Shi L L,Xu J,Li Y,Ma E.J Mater Res,2006;21: 2204 [27]Zheng Q,Ma H,Ma E,Xu J.Scr Mater,2006;55:541 [28]Zhang L,Zhuo M J,Xu J.J Mater Res,2008;23:688 [29]Zhang L,Ma E,Xu J.Intermetallics,2008;16:584 [30]Zhang Z X,Dai C L,Xu J.J Mater Sci Technol,2008;in press [31]Lin X H,Johnson W L.J Appl Phys,1995;78:6514 [32]Massalski T B.Binary Alloy Phase Diagrams.2 Ed.,Met- als Park,OH:ASM International,1996:1495 [33]Louzguine D V,Katao H D,Louzguina L V,Inoue A.J Mater Res,2004;19:3600 [34]Chen H S.Acta Metall,1976;24:153 [35]Miracle D B.Nature Mater,2004;3:697 [36]Guo F Q,Poon S J,Shiflet G J.J Appl Phys,2004;97: 013512 [37]Wang A P,Wang J Q.J Mater Res,2007;22:1 [38]Schuster J C,Naka M,Shibayanagi T.J Alloys Compd, 2000;305:L1 [39]Niessen A K,de Boer F R,Boom R,de Chatel P F,Mat- tens W C M,Miedema A R.Calphad,1983;7:51 [40]Wang D,Tan H,Li Y.Acta Mater,2005;53:2969 [41]Dai C L,Deng J W,Zhang Z X,Xu J.J Mater Res,2008; 23:1249 [42]Dai C L,Guo H,Li Y,Xu J.J Non-Cryst Solids,2008; 354:3659 |