| INVERSE ANALYSIS METHOD TO DETERMINE KINETICS FOR STATIC RECRYSTALLIZATION USING FLOW CURVES |
| ;; |
| 燕山大学机械工程学院 |
|
Cite this article:
. INVERSE ANALYSIS METHOD TO DETERMINE KINETICS FOR STATIC RECRYSTALLIZATION USING FLOW CURVES. Acta Metall Sin, 2008, 44(7): 837-842 .
|
|
|
Abstract The flow curves are obtained using single-hit and double-hit hot compression tests carried out on Gleeble-3500 thermomechanical simulator. The change of dislocation density during inter-pass is related to the static recrystallization volume fraction, which can be seen as a function of time. Based on the inverse analysis of the flow curves, a new method to estimate the kinetics for static recrystallization is proposed. Conventional approach using image analyses of quenched microstructure to evaluate the kinetics for static recrystallization can be replaced from this method. The proposed method is applied to the hot compression tests of plain carbon steel, and the kinetics for static recrystallization are obtained successfully for some range of deformation at elevated temperature. The results are clarified by comparing them with that reported in the literature. It is confirmed that the proposed method could provide accurate kinetics for static recrystallization with shorter time for experiment and computation.
|
|
Received: 06 December 2007
|
|
|
[1]Kwon O.ISIJ Int,1992;32:350 [2]McQueen H J,Yue S,Ryan N D,Fry E.J Mater Process Technol,1995;53:293 [3]Yoshie A,Morikawa H,Onoe Y,Itoh K.Trans Iron Steel Inst Jpn,1987;27:425 [4]Yanagimoto J,Liu J S.ISIJ Int,1999;39:171 [5]Senuma T,Yada H,Matsumura Y,Futamura T.Tetsu Hagané,1984;70:2112 (濑沼武秀,矢田浩,松村义一,二村忠.铁钢,1984;70:2112) [6]Chan J W.Acta Metall,1956;4:449 [7]Yanagimoto.J Mod Simul Mater Sci Eng,2002;10:111 [8]Yanagida A,Yanagimoto J.J Mater Process Technol, 2004;151:33 [9]Yoshie A,Fujita T,Fujioka M,Okamoto K,Morikawa H. ISIJ Int,1996;36:474 [10]Poliak E I,Jonas J J.Acta Metall,1996;44:127 [11]Ryan N D,McQueen H J.Can Metall Q,1990;29:147 [12]Mecking H,Kocks U F.Acta Metall,1981;29:1865 [13]Sun W P,Hawbolt E B.ISIJ Int,1997;37:1000 [14]Glowacki M,Kuziak P,Pietrzyk M.J Mater Process Tech- nol,1995;53:159 [15]Cabrera J M,Alomar A,Prado J M,Jonas J J.Metall Mater Trans,1997;28A:2233 [16]Karhausen K,Kopp R.Scand J Metall,1991;20:351 [17]Roberts W,Sandberg A,Siwecki T,Warlefors T.In:Proc Int Conf on HSLA Steels Technology and Applications, Philadelphia,ASM,1983:67 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|