| EFFECT OF SAMPLE ORIENTATION ON STATIC RECRYSTALLIZATION OF AZ31 MAGNESIUM ALLOY |
| HUANG Hongtao1, Godfrey Andrew1, LIU Wei1, TANG Ruihe1, LIU Qing2 |
1.Department of Materials Science and Engineering, Tsinghua University, Beijing 100084
2.School of Materials Science and Engineering, Chongqing University, Chongqing 400044 |
|
Cite this article:
HUANG Hongtao Godfrey Andrew LIU Wei TANG Ruihe LIU Qing. EFFECT OF SAMPLE ORIENTATION ON STATIC RECRYSTALLIZATION OF AZ31 MAGNESIUM ALLOY. Acta Metall Sin, 2012, 48(8): 915-921.
|
|
|
Abstract The effect of sample orientation on static recrystallization (SRX) of AZ31 magnesium alloy was investigated with electron backscattered diffraction (EBSD) technique. Two kinds of samples, one was cut along the normal direction of the sheet (0? sample), the other along the transverse direction of the sheet (90? sample), were given 15% uniaxial compression strain at 150℃, followed by annealing at 275℃ for different times. The results show that slip dominates the deformation process during 15% uniaxial compression strain for the 0? samples. However, extension twinning firstly dominates the deformation process and then slip dominates the deformation process during 15% uniaxial compression strain for the 90? samples. Due to the different deformation mechanisms, the deformation stored energy of the 90? samples is lower than that of the 0? samples. As a result, the initiation and completion of SRX of the 90? samples are significantly retarded compared with that of the 0? samples. As SRX proceeds, the percentage of low angle grain boundaries between 2? and 4? decreases dramatically and a peak located around 30? appears in misorientation angle distribution map for both the 90? samples and the 0? samples. Most SRX grains nucleate at the original grain boundaries for both the samples. A few SRX grains nucleate within extension twins.
|
|
Received: 27 March 2012
|
|
|
| Fund: Supported by National Basic Research Program of China (No.2007CB613703) |
| [1] Beer A G, Barnett M R. Mater Sci Eng, 2008; A485: 318[2] Robson J D, Henry D T, Davis B. Acta Mater, 2009; 57: 2739[3] Li X, Yang P, Wang L N, Meng L, Cui F. Mater Sci Eng, 2009; A517: 160[4] Yi S B, Schestakow I, Zaefferer S. Mater Sci Eng, 2009; A516: 58[5] Jager A, Lukac P V. Gartnerova V, Haloda J, Dopita M. Mater Sci Eng, 2006; A432: 20[6] Huang X S, Suzuki K, Chino Y. J Alloys Compd, 2011; 509: 4854[7] Mackenzie L W F, Pekguleryuz M. Mater Sci Eng, 2008; A480: 189[8] Liu Q. Acta Metall Sin, 2010; 46: 1458(刘庆. 金属学报, 2010; 46: 1458)[9] Perez–Prado M T, Ruano O A. Scr Mater, 2002; 46: 149[10] Perez–Prado M T, Ruano O A. Scr Mater, 2003; 48: 59[11] Jiang J, Godfrey A, Liu W, Liu Q. Mater Sci Eng, 2008; A483: 576[12] Humphreys F J, Hatherly M. Recrystallization and Related Annealing Phenomena. 2Ed., Oxford: Pergamon Press, 2004: 222[13] Huang H T, Liu W, Godfrey A, Tang R H, Liu Q. Acta Metall Sin, 2012; 48: 357(黄洪涛, 刘伟, Godfrey A, 唐瑞鹤, 刘庆. 金属学报, 2012; 48: 357)[14] Yang X Y, Zhang L. Acta Metall Sin, 2009; 45: 1303(杨续跃, 张雷. 金属学报, 2009; 45: 1303)[15] Wang M Y, Xin R L, Wang B S, Liu Q. Mater Sci Eng, 2011; A528: 2941[16] Brown D W, Agnew S R, Bourke M A M, Holden T M, Vogel S C, Tome C N. Mater Sci Eng, 2005; A399: 1[17] Clausen B , Tom´e C N, Brown D W, Agnew S R. Acta Mater, 2008; 56: 2456[18] Li X, Yang P, Meng L, Cui F E. Acta Metall Sin, 2010;46: 147(李萧, 杨平, 孟利, 崔凤娥. 金属学报, 2010; 46: 147)[19] Al–Samman T, Molodov K D, Molodov D A, Gottstein G, Suwas S. Acta Mater, 2012; 60: 537[20] Galiyev A, Kaibyshev R, Gottstein G. Acta Mater, 2001; 49: 1199[21] Jin Q L, Shim S Y, Lim S G. Scr Mater, 2006; 55: 843[22] Stanford N, Geng J, Chun Y B, Davies C H J, Nie J F, Barnett M R. Acta Mater, 2012; 60: 218[23] Barnett M R, Keshavarz Z, Ma X. Metall Mater Trans, 2006; 37A: 2283[24] Al–Samman T, Gottstein G. Mater Sci Eng, 2008; A490: 411 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|