| Microstructure transition from primary ε phase to peritectic η phase in Cu-75%Sn peritectic alloy under laser rapid solidification |
| 西北工业大学大学凝固技术国家重点实验室 |
|
Cite this article:
. Microstructure transition from primary ε phase to peritectic η phase in Cu-75%Sn peritectic alloy under laser rapid solidification. Acta Metall Sin, 2008, 44(7): 843-847 .
|
|
|
|
|
Received: 06 December 2007
|
|
|
[1]Umeda T,Okane T,Kurz W.Acts Mater,1996;44:4209 [2]Vandyoussefi M,Kerr H W,Kurz W.Acts Mater,2000; 48:2297 [3]Ma D,Li Y,Ng S C,Jones H.Acts Mater,2000;48:1741 [4]Su Y Q,Liu C,Li X Z,Guo J J,Li B S,Jia J,Fu H Z. Intermetallics,2005;13:267 [5]Shibata H,Arai Y,Suzuki M,Emi T.Metall Mater Trans, 2000;31B:981 [6]Li S M,Ma B L,LüH Y,Liu L,Fu H Z.Acts Metall Sin, 2005;41:411 (李双明,马伯乐,吕海燕,刘林,傅恒志.金属学报,2005;41:411) [7]LüH Y,Li S M,Liu L,Fu H Z.Spec Cast Nonferrous Alloys,2006;26:753 (吕海燕,李双明,刘林,傅恒志.特种铸造及有色合金,2006;26:753) [8]LüH Y,Li S M,Liu L,Fu H Z.Sci China,2007;50G:451 [9]Su Y P,Wang M,Lin X,Li H L,Huang W D.Acts Metall Sin,2005;41:67 (苏云鹏,王猛,林鑫,李华琳,黄卫东.金属学报,2005;41:67) [10]Xu W,Feng Y P,Li Y,Zhang G D,Li Z Y.Acts Mater, 2002;50:183 [11]Duan G H,Liu Y C,Yang G C,Zhou Y H.Mater Left, 2003;57:1091 [12]Kerr H W,Kurz W.Int Mater Rev,1996;41:129 [13]Kubin L P,Estrin Y.Acts Metall,1985;33:397 [14]Kurz W,Fisher D J.Fundamentals of Solidification.4th Ed.,Switzerland:Trans Tech Publications Ltd,1998:201 [15]Trivedi R,Kurz W.Metall Trans,1990;21A:1311 [16]Fredriksson H,Nylen T.Met Sci,1982;16:283 [17]Saunders N,Miodownik A P.Phase Diagrams of Binary Copper Alloys.Materials Park,OH:ASM International, 1994:412 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|