| EFFECT OF RE (RARE EARTH) ON THE CORROSION RESISTANCE OF CARBON STEEL IN 0.3 mol/L NACL SOLUTION |
| ;;;;;; |
| 钢铁研究总院 |
|
Cite this article:
. EFFECT OF RE (RARE EARTH) ON THE CORROSION RESISTANCE OF CARBON STEEL IN 0.3 mol/L NACL SOLUTION. Acta Metall Sin, 2008, 44(7): 863-866 .
|
|
|
Abstract The corrosion process of RE steel and carbon steel in 0.3 mol/L NaCl was investigated by electrochemistry impedance spectroscopy test, SEM and X diffraction analysis. The results showed RE could improve the corrosion resistance of carbon steel; compared with carbon steel, the rust layer of RE steel generated in the solution was more compact, the content of α-FeOOH in rust layer with protective effect was higher, the content of activated γ-FeOOH and β-FeOOH was little. The development process of electrochemistry parameter in the equivalent circuit was analysed, the theory of RE improving the corrosion resistance of steel was discussed.
|
|
Received: 10 October 2007
|
|
|
[1]Zhang H,Zhang F S.Steelmaking,2003;19(4):19 (张化,章奉山.炼钢,2003;19(4):19) [2]Chen J Q,Chen B W,Hu M,Song Y L.Res Iron Steel, 2003;31(5):49 (陈吉清,陈邦文,胡敏,宋育来.钢铁研究,2003;31(5):49) [3]Wang L M,Du T,Wang Y K.J Chin Rare Earth Soc, 2003;21:491 (王龙妹,杜挺,王跃奎.中国稀土学报,2003;21:491) [4]Zhang H W,Mao Y W,Sun M H,Yu Z S.J Univ Sci Technol Beijing,1994;16:491 (张蕙文,毛裕文,孙明华,余宗森.北京科技大学学报,1994;16:491) [5]Lin Q,Chen B W,Guo F,Guo Y,Sun X Y,Zhang Z P. Chin Rare Earths,2003;24(5):26 (林勤,陈帮文,郭锋,郭英,孙学义,张志平.稀土,2003;24(5):26) [6]Yue L J,Wang L M,Piao X Y,Xu C H,Zhu J X.J Iron Steel Res,2006;18:34 (岳丽杰,王龙妹,朴秀玉,徐成海,朱京希.钢铁研究学报,2006;18:341 [7]Li C Y,Wang X D,Jiang S M,Chen X P,Weng Y,Zhang J B,Zhang D M.Chin Rare Earths,2005;26(6):23 (李春艳,王向东,江社明,陈小平,翁宇,张静波,张代明.稀土,2005;26(6):23) [8]Yang Z N,Zhang Z,Su J X,Zhang J Q,Li Z G,Yang A N,Cao C N.Acta Metall Sin,2005;41:860 (杨仲年,张昭,苏景新,张鉴清,李自刚,杨阿娜,曹楚南.金属学报,2005;41:860) [9]Dillmann P,Mazaudier F,Hoerle S.Corros Sci,2004;46: 1401 [10]Takenori N,Fumio Y,Haruya K.R&D Kobe Steel Eng Rep,2001;51:29 [11]Hinton B R W,Arnott D R,Ryan N E.Met Forum,1984; 7:211 [12]Hinton B R W,Arnott D R,Ryan N E.Mater Forum, 1986;9:162 [13]Goldie B P F,McCarroll J J.Aust Pat,AU-32947/84, 1984 [14]Chu Y Y,Zhao L.Identifying of RE Inclusion in Steel. Beijing:Metallurgical Industry Press,1985:18 (褚幼义,赵琳.钢中稀土夹杂物鉴定.北京:冶金工业出版社,1985:18) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|