| VERIFICATION OF THREE 3D INDIVIDUAL GRAIN GROWTH RATES WITH LARGE-SCALE MONTE CARLO SIMULATION |
| ;; |
| 北京科技大学 |
|
Cite this article:
. VERIFICATION OF THREE 3D INDIVIDUAL GRAIN GROWTH RATES WITH LARGE-SCALE MONTE CARLO SIMULATION. Acta Metall Sin, 2008, 44(1): 13-18 .
|
|
|
Abstract Three existing topological dependence equations for the growth rate of three-dimensional individual grains have been testified using a new Potts model Monte Carlo simulation. The result shown that the volume change rate dVf/dt is related to the face number f by a curve, and thus, Rivier’s grain growth rate equation that predicts dVf/dt ∝f is not confirmed. Yu-Liu’s grain growth rate equation and MacPherson-Srolovitz’s grain growth rate equation are confirmed by mean of the simulation in the case of the face number f≥8. Yu-Liu’s grain growth rate equation and MacPherson-Srolovitz’s grain growth rate equation are not valid in the case of the face number f<8.
|
|
Received: 28 May 2007
|
|
|
[1]Beck P A,Holaworth M L,Hu H.Phys Rev,1948;73:526 [2]Burke J E.Trans AIME,1949;180:73 [3]Turnbull D.Trans AIME,1951;191:661 [4]von Neumann J.In:Herring C,ed.,Metal Interfaces, Cleveland,American Society for Metals,1952:108 [5]Mullins W W.In:Robertson W D,Gjostein N A,eds., Metal Surfaces:Structure,Energetics,and Kinetics,Met- als Park,OH:American Society for Metals,1963:17 [6]Mullins W W.J Appl Phys,1956;27:900 [7]Rivier N.Philos Mag,1983;47B:245 [8]Yu H B,Liu G Q.Chin Sci Bull,1996;41:2000 (于海波,刘国权.科学通报,1996;41:2000) [9]Liu G Q,Yu H B,Song X Y,Qin X G.Mater Des,2001; 22:33 [10]Liu G Q,Song X Y,Yu H B,Gu N J.Acta Metall Sin, 1999;35:245 (刘国权,宋晓艳,于海波,谷南驹.金属学报,1999;35:245) [11]Wang C,Liu G Q,Yu H B.Acta Metall Sin,2004;40: 1233 (王超,刘国权,于海波.金属学报,2004;40:1233) [12]MacPherson R D,Srolovitz D J.Nature,2007;446:1053 [13]Qin X G.Doctorate Dissertation,University of Science and Technology Beijing,2003 (秦湘阁.北京科技大学博士学位论文,2003) [14]Glazier J A.Phys Rev Lett,1993;70:2170 [15]Radhakrishnan B,Zacharia T.Metall Mater Trans,1995; 26A:167 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|