| Gas Pressure Condition for Obtaining Uniform Lotus--Type Porous Structure by Gasar Process |
| ZHANG Huawei; LI Yanxiang; LIU Yuan |
| Key Laboratory for Advanced Materials Processing Technology; Ministry of Education; Department of Mechanical Engineering; Tsinghua University; Beijing; 100084 |
|
Cite this article:
ZHANG Huawei; LI Yanxiang; LIU Yuan. Gas Pressure Condition for Obtaining Uniform Lotus--Type Porous Structure by Gasar Process. Acta Metall Sin, 2006, 42(11): 1171-1176 .
|
|
|
Abstract Gas pressure is the effective and most easily controlled parameter for fabricating lotus-type porous metals with long cylindrical regular ordered pores by unidirectional solidification of metal-gas eutectic. The kind of gas which is applicable for Gasar process was discussed in this article. Gas pressure condition for obtaining uniform lotus-type porous structure in which the spatial distribution and the size of pores both are highly uniform has been established through analyzing the influence of gas pressure on the position of eutectic point and solidification mode (eutectic, hypereutectic and hypoeutectic mode), and comparing the homogeneity of lotus-type porous structures obtained under three solidification mode. As an example, the experimental results of magnesium and hydrogen system verified the above theory.
|
|
Received: 28 March 2006
|
|
|
[1] Shapovalov V I. US Pat, 5 181 549, 1993 [2] Shapovalov V I. MRS Bull, 1994; 4: 24 [3] Liu Y, Li Y X, Wan J, Zhang H W. Mater Sci Eng, 2005; A402: 47 [4] Li Y X, Liu Y, Zhang H W, Wang X. In: Nakajima H, Kanetake N eds., Proceedings of Metal Foam 2005, Osaka: The Japan Institute of Metals, 2006: 237 [5] Shapovalov V I, Boyko L. Adv Eng Mater, 2004; 6: 407 [6] Wolla J M, Provenzano V. Mater Res Soc Symp Proc, 1995; 371: 377 [7] Kovacik J. Acta Mater, 1998; 46: 5413 [8] Simone A E, Gibson L J. Acta Mater, 1996; 44: 1463 [9] Hyun S K, Murakami K, Nakajima H. Mater Sci Eng, 2001; A299: 241 [10] Xie Z K, Ikeda T, Okuda Y, Nakajima H. Mater Sci Eng, 2004; A386: 390 [11] Xie Z K, Ikeda T, Okuda Y, Nakajima H. Mater Sci Forum, 2004; 449-452: 661 [12] Ogushi T, Chiba H, Nakajima H, Ikeda T. J Appl Phys, 2004; 95: 5843 [13] Tane M, Hyun S K, Nakajima H. J Appl Phys, 2005; 97: 103701 [14] Liu Y, Li Y X, Zhang H W, Wan J. Acta Metall Sin, 2005; 41: 886 (刘源,李言祥,张华伟,万疆.金属学报,2005;41:886) [15] Liu Y, Li Y X, Zhang H W, Wan J. Rare Met Mater Eng, 2005; 34: 1128 (刘源,李言祥,张华伟,万疆.稀有金属材料与工程, 2005;34:1128) [16] Liu Y, Li Y X, Zhang H W. Acta Metall Sin, 2004; 40: 1121 (刘源,李言祥,张华伟.金属学报, 2004;40:1121) [17] Xie Z K, Ikeda T, Okuda Y, Nakajima H. Mater Sci Forum, 2004; 449-452: 661 [18] Nakajima H, Hyun S K, Ohashi K, Ota K, Murakami K. Colloids Surf, 2001; A179: 209 [19] Suematsu Y, Hyun S K, Nakajima H. J Jpn Inst Met, 2004; 68: 257 (末松佳记,玄丞均,中屿英雄.日本金属学会志, 2004;68: 257) [20] Ikeda T, Aoki T, Nakajima H. Metall Mater Trans, 2005; A36: 77 (玄丞均,池田辉之,中(?)英雄.日本金属学会志, 2004;68: 39) [21] Nakahata T, Nakajima H. Mater Sci Eng, 2004; A384: 373 [22] Hyun S K, Ikeda T, Nakajima H. J Jpn Inst Met, 2004; 68: 39 [23] Hyun S K, Ikeda T, Nakajima H. Sci Technol Adv Mater, 2004; 5: 201 [24] Hyun S K, Nakajima H. Adv Eng Mater, 2002; 4: 741 [25] Nakahata T, Nakajima H. Mater Trans, 2005; 46: 587 [26] Yasuda H, Ohnaka I, Dhindaw B W, Takezawa N, Fujimoto S, Nagira T, Tsuchiyama A, Nakano T, Uesugi K. In: Nakajima H, Kanetake N, eds., Proceedings of Met Foam 2005, Osaka: The Japan Institute of Metals, 2006: 289 [27] Liu Y, Li Y X, Zhang H W, Wan J. Spec Cast Nonferrous Alloy, 2005; 25: 1 (刘源,李言祥,张华伟,万疆.特种铸造及有色合金, 2005;25:1) [28] An G Y. Formation Theory of Castings. Beijing: China Machine Press, 1989: 173 (安阁英.铸件形成理论.北京:机械工业出版社,1989:173) [29] Shapovalov V I, Semik A P, Timchenko A G. Russ Metall, 1993; (3): 21 [30] Yamamura S, Shiota H, Murakami K. Mater Sci Eng, 2001; A318: 137 [31] Schwarz H, Exner H E. J Microsc, 1983; 129: 155 [32] Zhang H W, Li Y X, Liu Y. Acta Metall Sin, 2005; 41: 55 (张华伟,李言祥,刘源.金属学报, 2005;41:55) [33] Liu Y, Li Y X, Wan J, Zhang H W. In: Nakajima H, Kanetake N eds., Proceedings of Met Foam 2005, Osaka: The Japan Institute of Metals, 2006: 241 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|