Abstract Nikel nanowires were prepared by direct current electrodeposition within the nanopores of anodic alumina membrane (AAM). The topography and texture of the nanowires were characterized by SEM, XRD, TEM. It is found that the nickel nanowires are the structure of single crystalline with a preferred orientation along the [111] direction. It is demonstrated that the nickel nanowires are dielectrical dissipation materials in the microwave electromagnetic experiment, the value of dielectrical dissipation is 0.55 at 9.5GHz. The nickel nanowires are considered as a candidate for microwave absorbing material.
|
Received: 14 July 2006
|
|
[1] Prida V M,Hernandez—Velez M,Cervera M,Pirota K, Sanz R,Navas D,Asenjo A,Aranda P,Ruiz—Hitzky E, Batallan F,Vazquez M,Hernando B,Menendez A,Bor—del N,Pereiro R.J Magn Magn Mater,2005;294:e69 [2] Pau G P,Xue K H,Sun D M,Xu S M,Pan M H,Lu M, Qiu Q,Li G L,Wang G H. Chin J Chem Phys,1999;12: 675 (潘谷平,薛宽宏,孙冬梅,徐土民,潘明虎,鹿牧,邱齐,李光来,王广厚.化学物理学报, 1999;12:675) [3] Qin J,Nogues J,Mikhaylova M,Roig A,Munoz J S, Muhammed M.Chem Mater, 2005;l7:1829 [4] Pan H,Liu B,Yi J,Poh C,Lim S,Ding J,Feng Y P.Huan C H A, Lin J.J Phys Chem, 2005;109B:3094 [5] Hu C X.Technology of Coating Stealth.Beijing:Chemical Industry Press,2004:276 (胡传炘.隐身涂层技术.北京:化学工业出版社,2004:276) [6] Peng W C,Chen K H,Li J L,Huang L P. Chin J Non—ferrous Met, 2005;2:288 (彭伟才,陈康华,李晶儡,黄兰萍.中国有色金属学报,2005, 2:288) [7] Meng H.Mod Paint Finish,2005;8(6):8 (孟辉.现代涂料与涂装,2005;8(6):8) [8] Rahman I z,Boboc A,Razeeb K M,Rahman M A.J Magn Magn Mater,2005;290 291:246 [9] Zhang X Y,Xu L H,Dai J Y,Chan H L W.Physica,2004; 353B:187 [10] Chen M,Chien C L,Searson P C.Chem Mater,2006;18: 1595 [11] Liu J H,Yu M,Li S M.Chin J Inorg Chem,2005;2l:429 (刘建华,于美,李松梅.无机化学学报, 2005; 21:429) [12] Yu M,Liu J H,Li S M,Wei W.J Inorg Mater,2005;20: 1363 (于美,刘建华,李松梅,韦巍.无机材料学报,2005;20: 1363) [13] Li s M,Chen D M,Liu J H.Acta Phys-Chim Sin,2004; 20:1389 (李桦梅,陈冬梅,刘建华.物理化学学报, 2004;20:1389) [14] Hiheki M,Kenji F.Science,1995;268:1466 [15] Miura K,Masuda M,Itoh M,Horikawa T,Machida K.J Alloys Compd, 2006;408-412:139 |
No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
|
Shared |
|
|
|
|
|
Discussed |
|
|
|
|