| STUDY ON REHYDROGENATION OF THE DECOMPOSED NaAlH4 |
| SUN Dalin;;;; |
| 复旦大学 |
|
Cite this article:
SUN Dalin. STUDY ON REHYDROGENATION OF THE DECOMPOSED NaAlH4. Acta Metall Sin, 2007, 42(1): 96-98 .
|
|
|
Abstract In-situ X-ray diffraction showed that Ti catalyst can reduce not only the dehydrogenation temperature of NaAlH4, but also that of Na3AlH6 from 250 ℃ to 160 ℃. The rehydrogenation of the decomposed NaAlH4 is reversible theoretically, but the intermediate hydride, Na3AlH6, is not fully converted into NaAlH4 because of the physical separation of NaH and Al formed in the decomposition, especially the formation of the large Al crystallites. These, therefore, result in a decrease in the hydrogen storage capacity as observed in the following cycling. Additional measurements have showed that those Al crystallites larger than 2.3 µm are no longer effective for rehydrogenatrion.
|
|
Received: 24 May 2006
|
|
|
[1]Jenson C M,Gross K J.Appl Phys,2001;72A:213 [2]Bogdanovic B,Schwickardi M.J Alloys Compd,1997;253: 1 [3]Sun D L,Chen G R,Jiang J J,Lei Y Q,Wang Q D.Mater Rev,2004;18(5):72 (孙大林,陈国荣,江建军,雷永泉,王启东.材料导报,2004; 18(5):72) [4]Sun D L,Srinivasan S S,Chen G R,Jensen C M.J Alloys Compd,2004;373:265 [5]Gross K J,Sandrock G,Thomas G J.J Alloys Compd, 2002;330:691 [6] Gross K J,Guthrie S,Takara S,Thomas G. J Alloy Compd,2000;297:270 [7] Sun D L,Kiyobayashi T,Takeshita H T,Kuriyama N, Jensen C M.J Alloys Compd.2002; 337:L8 [8]Srinivasan S S,Brinks H W,Hauback B C,Jensen C M. J Alloys Compd,2004;377:283 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|