STUDY ON ELECTROMAGNETIC PROPERTY FOR MICROWAVE ABSORBING OF NICKEL NANOWIRES
YU;;
北京航空航天大学
Cite this article: 

YU. STUDY ON ELECTROMAGNETIC PROPERTY FOR MICROWAVE ABSORBING OF NICKEL NANOWIRES. Acta Metall Sin, 2007, 42(1): 99-102 .

Download:  PDF(242KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Nikel nanowires were prepared by direct current electrodeposition within the nanopores of anodic alumina membrane (AAM). The topography and texture of the nanowires were characterized by SEM, XRD, TEM. It is found that the nickel nanowires are the structure of single crystalline with a preferred orientation along the [111] direction. It is demonstrated that the nickel nanowires are dielectrical dissipation materials in the microwave electromagnetic experiment, the value of dielectrical dissipation is 0.55 at 9.5GHz. The nickel nanowires are considered as a candidate for microwave absorbing material.
Key words:  nickel nanowires      anodic alumina membrane      electrodeposition      microwave electromagnetic property      
Received:  14 July 2006     
ZTFLH:  O488  
  TM27  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors
YU

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V42/I1/99

[1] Prida V M,Hernandez—Velez M,Cervera M,Pirota K, Sanz R,Navas D,Asenjo A,Aranda P,Ruiz—Hitzky E, Batallan F,Vazquez M,Hernando B,Menendez A,Bor—del N,Pereiro R.J Magn Magn Mater,2005;294:e69
[2] Pau G P,Xue K H,Sun D M,Xu S M,Pan M H,Lu M, Qiu Q,Li G L,Wang G H. Chin J Chem Phys,1999;12: 675 (潘谷平,薛宽宏,孙冬梅,徐土民,潘明虎,鹿牧,邱齐,李光来,王广厚.化学物理学报, 1999;12:675)
[3] Qin J,Nogues J,Mikhaylova M,Roig A,Munoz J S, Muhammed M.Chem Mater, 2005;l7:1829
[4] Pan H,Liu B,Yi J,Poh C,Lim S,Ding J,Feng Y P.Huan C H A, Lin J.J Phys Chem, 2005;109B:3094
[5] Hu C X.Technology of Coating Stealth.Beijing:Chemical Industry Press,2004:276 (胡传炘.隐身涂层技术.北京:化学工业出版社,2004:276)
[6] Peng W C,Chen K H,Li J L,Huang L P. Chin J Non—ferrous Met, 2005;2:288 (彭伟才,陈康华,李晶儡,黄兰萍.中国有色金属学报,2005, 2:288)
[7] Meng H.Mod Paint Finish,2005;8(6):8 (孟辉.现代涂料与涂装,2005;8(6):8)
[8] Rahman I z,Boboc A,Razeeb K M,Rahman M A.J Magn Magn Mater,2005;290 291:246
[9] Zhang X Y,Xu L H,Dai J Y,Chan H L W.Physica,2004; 353B:187
[10] Chen M,Chien C L,Searson P C.Chem Mater,2006;18: 1595
[11] Liu J H,Yu M,Li S M.Chin J Inorg Chem,2005;2l:429 (刘建华,于美,李松梅.无机化学学报, 2005; 21:429)
[12] Yu M,Liu J H,Li S M,Wei W.J Inorg Mater,2005;20: 1363 (于美,刘建华,李松梅,韦巍.无机材料学报,2005;20: 1363)
[13] Li s M,Chen D M,Liu J H.Acta Phys-Chim Sin,2004; 20:1389 (李桦梅,陈冬梅,刘建华.物理化学学报, 2004;20:1389)
[14] Hiheki M,Kenji F.Science,1995;268:1466
[15] Miura K,Masuda M,Itoh M,Horikawa T,Machida K.J Alloys Compd, 2006;408-412:139
[1] HANG Tao, XUE Qi, LI Ming. A Review on Metal Micro-Nanostructured Array Materials Routed by Template-Free Electrodeposition[J]. 金属学报, 2022, 58(4): 486-502.
[2] GAO Yunming, HE Lin, QIN Qingwei, LI Guangqiang. ZrO2 Solid Electrolyte Aided Investigation on Electrodeposition in Na3AlF6-SiO2 Melt[J]. 金属学报, 2022, 58(10): 1292-1304.
[3] GAO Bowen, WANG Meihan, YAN Maocheng, ZHAO Hongtao, WEI Yinghua, LEI Hao. Electrochemical Preparation and Corrosion Resistance of PEDOT Coatings on Surface of 2024 Aluminum Alloy[J]. 金属学报, 2020, 56(11): 1541-1550.
[4] Mingyu ZHAO,Huijuan ZHEN,Zhihong DONG,Xiuying YANG,Xiao PENG. Preparation and Performance of a Novel Wear-Resistant and High Temperature Oxidation-Resistant NiCrAlSiC Composite Coating[J]. 金属学报, 2019, 55(7): 902-910.
[5] Zhao CHENG, Shuai JIN, Lei LU. Effect of Electrolyte Temperature on Microstructures of Direct-Current Electrodeposited Nanotwinned Cu[J]. 金属学报, 2018, 54(3): 428-434.
[6] Tingting ZHAO, Zhixin KANG, Xiayu MA. Fabricating Superhydrophobic Copper Meshes by One-Step Electrodeposition Method and Its Anti-Corrosion and Oil-Water Separation Abilities[J]. 金属学报, 2018, 54(1): 109-117.
[7] Shuai JIN,Zhao CHENG,Qingsong PAN,Lei LU. EFFECT OF ELECTROLYTE ADDITIVE CONCEN-TRATION ON MICROSTRUCTURE OF DIRECT-CURRENT ELECTRODEPOSITED NANOTWINNED Cu[J]. 金属学报, 2016, 52(8): 973-979.
[8] SHAN Haiquan, ZHANG Yuefei, MAO Shengcheng, ZHANG Ze. ELECTRON MICROSCOPY STUDY OF FIVE-FOLD TWINS IN ELECTRODEPOSITED NANO-TWIN Ni[J]. 金属学报, 2014, 50(3): 305-312.
[9] LI Xuliang, ZHANG Yingchun, JIANG Fan, WANG Lili, LIU Yanhong, SUN Ningbo. EFFECTS OF CURRENT DENSITY ON MICROSTRUCTURE OF W COATING ON V-4Cr-4Ti ALLOY BY ELECTRODEPOSITION[J]. 金属学报, 2013, 49(6): 745-750.
[10] NIU Yunsong, WEI Jie, ZHAO Jian, HU Jiaxiu, YU Zhiming. PREPARATION AND PROPERTIES OF NANOSIZED MUL-TILAYERED Ni COATINGS BY ULTRASOUND-ASSISTED ELECTRODEPOSITION[J]. 金属学报, 2013, 49(12): 1617-1622.
[11] LONG Qiong, ZHONG Yunbo, LI Fu, LIU Chunmei, ZHOU Junfeng, FAN Lijun, LI Mingjie. EFFECT OF STATIC MAGNETIC FIELD ON THE MORPHOLOGY AND Si CONTENT OF Fe-Si COMPOSITE COATING[J]. 金属学报, 2013, 49(10): 1201-1210.
[12] CHENG Yuhao ZHANG Yuefei MAO Shengcheng HAN Xiaodong ZHANG Ze. EFFECT OF TEMPERATURE ON MICROSTRUCTURE AND NANOINDENTATION MECHANICAL PROPERTIES OF ELECTRODEPOSITED NANO-TWINNED Ni[J]. 金属学报, 2012, 48(11): 1342-1348.
[13] ZHANG Hao WU Di ZHANG Li DUAN Zhenzhen LAI Chi–Ming LIU Zhiquan . WAFER LEVEL ELECTRODEPOSION OF Fe–Ni NOVEL UBM FILMS[J]. 金属学报, 2012, 48(10): 1273-1280.
[14] LI Wenchuan CAI Jun LING Guoping. Al-Cr COATINGS PREPARED BY DIFFUSION AT LOW TEMPERATURE AND ITS PHASE CHARACTERIZATION[J]. 金属学报, 2011, 47(2): 231-235.
[15] ;. THE EFFECT OF MECHANICAL ATTRITION ON THE GRAIN GROWTH OF ELECTRODEPOSOTION Ni COATINGS[J]. 金属学报, 2008, 44(6): 751-756 .
No Suggested Reading articles found!