Please wait a minute...
Acta Metall Sin  2007, Vol. 42 Issue (1): 91-95     DOI:
Research Articles Current Issue | Archive | Adv Search |
The influences of pulsing current and isothermal annealing on the microstructure and micro-hardness of Fe73.5Cu1Nb3Si13.5B9 amorphous ribbons
;
清华大学
Cite this article: 

;. The influences of pulsing current and isothermal annealing on the microstructure and micro-hardness of Fe73.5Cu1Nb3Si13.5B9 amorphous ribbons. Acta Metall Sin, 2007, 42(1): 91-95 .

Download:  PDF(270KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The influence of pulsing current and isothermal annealing on the microstructure and micro-hardness of Fe73.5Cu1Nb3Si13.5B9 amorphous ribbons have been studied. It has been found that Fe73.5Cu1Nb3Si13.5B9 amorphous ribbons can significantly nanocrystallized by pulsing current treatment in a short processing time (within 30 s) at low processing temperature (100 K lower than glass transition temperature). At the early stage of pulsing current treatment, the micro-hardness increases by 10% from 8.2 to 9.0 GPa with respect to the initial ribbons, resulted by the structural relaxation. Then an abrupt increase by 50% from 8.2 to 12.4 GPa of the micro-hardness occur, as a result of the precipitation of abundant α-Fe nanocrystals with an average grain size of 8.5 nm. It indicates that pulsing current treatment is an effective way for the nanocrystallization of the studied amorphous alloy.
Key words:  pulsing current      nanocrystallization      micro-hardness      isothermal annealing      
Received:  17 April 2006     
ZTFLH:  TG139.8  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V42/I1/91

[1] Yoshizawa Y,Oguma S,Yamauchi K.J Appl Phys,1988; 64:6044
[2] Yoshizawa Y,Yamauchi K.Mater Trans JIM,1990;31: 307
[3] Hono K,Inoue A,Sakurai T.Appl Phys Lett,1991;58: 2180
[4] Herzer G.IEEE Trans Magn,1990;26:1397
[5] Ayers J D,Harris V G,Sprague J A,Elam W T,Jones H N.Acta Mater,1998;46:1861
[6] McHenry M E,Willard M A,Laughlin D E.Prog Mater Sci,1999;44:291
[7] Lai Z H,Conrad H,Chao Y S,Wang S G,Sun J.Scr Metall,1989;23:305
[8] Chao Y S,Sun S Q,Teng G Q,Lai Z H.Acta Phys Sin, 1996;45:1506 (晁月盛,孙少权,滕功清,赖祖涵.物理学报,1996;45:1506)
[9] Lai Z H,Conrad H,Teng G Q,Chao Y S.Mater Sci Eng, 2000;A287:238
[10] Houssa R,Franco V,Conde A.J Magn Magn Mater,1999; 203:199
[11] Wu W F,Yao K F,Zhao Z K.Chin Sci Bull,2004;49: 2268 (吴文飞,姚可夫,赵占奎.科学通报, 2004;49:2268)
[12] Zhang C Y,Yao K F.J Non—Cryst Solids,2005;351:3663
[13] Yao K F,Wang P Y.J Meeh Strength,2003;25:340 (姚可夫,王沛玉.机械强度, 2003;25:340)
[14]Wu W F,Yao K F.Rare Met Mater Eng,2005;34:505 (吴文飞,姚可夫.稀有金属材料与工程, 2005;34:505)
[15] Mizubayashi H,Hao T,Tanimoto H.J Non Cryst Solids, 2002;312-314:581
[16] Holland T B,Loffler J F,Munir Z.J Appl Phys, 2004;95: 2896
[17] Chen H S,Chuang S Y.Appl Phys Lett,1977;31:255
[18] Chen H S,Lo C C.In:Grant N J,Giessen B C,eds., proc 2nd Int Conf on Rapidly Quenched Metals, Cambridge. Mass.: Massachusetts Institute of technology Press.1976: 413
[19] Ba Q X,Zeng G Y,Xiong L Y,Zhou G Z.J Northeast Univ,1999;20:626 (巴启先,曾佳仪,熊良钺,周广智.东北大学学报. 1999;20: 626)
[20] Zou H,Wang J F,Liu L.Chin J Nonferrous Met,2004; 14:996 (邹辉,王敬丰,柳林.中国有色金属学报,2004:14:996)
[21] Chen H S,Inoue A,Masumoto T.J Mater Sci,1985;20: 2417
[22] Um C Y,Johnson F,Simone M,Barrow J,McHenry M E.J Appl Phys,2005;97:10F504
[23] Yao K F,Yu P,Zheng M X,Wang J,Zhang H T,Fang W, Sun J Z.Acta Metall Sin, 2000;36:630 (姚可夫,余鹏,郑明新,王俊,张华堂,方威,孙建周金属学报,2000;36:630)
[24] Yao K F,Wang J,Zheng M X,Yu P,Zhang H T.Sct Mater, 2001; 45:533
[25] Yao K F,Yu P,Wang J,Fang W,Zheng M X.Acta Metall Sin (Engl Lett),2001;14:341
[26] Yao K F,Yu P,Zheng M X.Tribology,2002;22:202 (姚可夫,余鹏,郑明新.摩擦学学报, 2002;22:202)
[27] Conrad H.Mater Sci Eng,2000;A287:227
[28] Conrad H.Mater Sci Eng,2000;A287:276L
[1] Jianhai YANG,Yuxiang ZHANG,Liling GE,Xiao CHENG,Jiazhao CHEN,Yang GAO. Effect of Hybrid Surface Nanocrystallization Before Welding on Microstructure and Mechanical Properties of Friction Stir Welded 2A14 Aluminum Alloy Joints[J]. 金属学报, 2017, 53(7): 842-850.
[2] Gang LIU, Chao LI, Ye MA, Ruijun ZHANG, Yongkai LIU, Yuhui SHA. HEAT STABILITY AND SILICONIZING BEHAVIOR OF SURFACE NANOSTRUCTURE OF SILICON STEEL INDUCED BY ASYMMETRIC ROLLING[J]. 金属学报, 2016, 52(3): 307-312.
[3] Jianhai YANG,Yuxiang ZHANG,Liling GE,Jiazhao CHEN,Xin ZHANG. EFFECT OF HYBRID SURFACE NANOCRYSTALLI-ZATION ON THE ELECTROCHEMICAL CORROSION BEHAVIOR IN 2A14 ALUMINUM ALLOY[J]. 金属学报, 2016, 52(11): 1413-1422.
[4] DING Jie, ZHANG Zhiming, WANG Jianqiu, HAN En-Hou, TANG Weibao, ZHANG Maolong, SUN Zhiyuan. MICRO-CHARACTERIZATION OF DISSIMILAR METAL WELD JOINT FOR CONNECTING PIPE- NOZZLE TO SAFE-END IN GENERATION III NUCLEAR POWER PLANT[J]. 金属学报, 2015, 51(4): 425-439.
[5] PU Sheng, XIE Guang, ZHENG Wei, WANG Dong, LU Yuzhang, LOU Langhong, FENG Qiang. EFFECT OF W AND Re ON DEFORMATION AND RECRYSTALLIZATION OF SOLUTION HEAT TREATED Ni-BASED SINGLE CRYSTAL SUPERALLOYS[J]. 金属学报, 2015, 51(2): 239-248.
[6] LIU Gang, MA Ye, ZHANG Ruijun, WANG Xiaolan, SHA Yuhui, ZUO Liang. SURFACE NANOCRYSTALLIZATION OF SILICON STEEL INDUCED BY ASYMMETRIC ROLLING AND EFFECT OF ROLLING PARAMETERS[J]. 金属学报, 2014, 50(9): 1071-1077.
[7] LIU Wenbo, ZHANG Chi, YANG Zhigang, XIA Zhixin, GAO Guhui, WENG Yuqing. EFFECT OF SURFACE NANOCRYSTALLIZATION ON MICROSTRUCTURE AND THERMAL STABILITY OF REDUCED ACTIVATION STEEL[J]. 金属学报, 2013, 49(6): 707-716.
[8] LIU Gang, LIU Jinyang,WANG Xiaolan,WANG Fuhui,ZHAO Xiang,ZUO Liang . FORMATION OF NANOCRYSTALLINES IN THE SURFACE LAYER OF COMMERCIAL PURE TITANIUM THIN SHEET DURING ASYMMETRIC ROLLING[J]. 金属学报, 2013, 49(5): 599-604.
[9] GONG Jing YANG Hongwang YANG Baijun WANG Ruichun LI Rongde WANG Jianqiang. MAGNETISM OF MONOLITHIC AND PARTIALLY CRYSTALLIZED AMORPHOUS Al–Ni–Y ALLOYS[J]. 金属学报, 2011, 47(3): 333-336.
[10] BAI Tao LI Dong GUAN Kaishu. PROPERTY  VARIATION AND MICRO-STRUCTURE EVOLUTION OF 304L STAINLESS STEEL SUBJECTED TO SURFACE MECHANICAL ROLLING TREATMENT[J]. 金属学报, 2011, 47(11): 1459-1463.
[11] . XRD Investigation of The Recrystallization Process of Shot Peened Layer on In-Situ TiB2/6351Al[J]. 金属学报, 2008, 44(6): 671-674 .
[12] LU Ni; uan; SONG Xiaoyan; ZHANG Jiuxing; LI Erdong. Preparation of Nd Bulk with Ultrafine Nanocrystalline Structure and its Physical Property[J]. 金属学报, 2007, 43(7): 739-743 .
[13] LI Sijun; LIU Gang; ZHOU Lei; WANG Fu; ZUO Liang. Evolutions of Structure, Texture And Mechanical Property of IF Steel Subjected to Surface Mechanical Attrition Treatment[J]. 金属学报, 2007, 43(7): 744-748 .
[14] Lin-Xiu DU. SUBMICRON-NANOCRYSTALLIZATION OF LOW CARBON STEELS THROUGH TRANSFORMATION MECHANISM[J]. 金属学报, 2007, 42(1): 59-63 .
[15] WANG Aixiang; LIU Gang; ZHOU Lei; WANG Ke; YANG Xiaohua; LI Ying. Thermal Stability of Structure and Hardness of the Surface Layer of 316L Stainless Steel After Surface Mechanical Attrition Treatment[J]. 金属学报, 2005, 41(6): 577-582 .
No Suggested Reading articles found!