THE PLASTIC DEFORMATION AND EFFECT OF HYDROGEN ON DEFORMATION OF Ni-P AMORPHOUS COATINGS
Qing-Jun Zhou;;;;;
北京科技大学材料物理与化学系
Cite this article: 

Qing-Jun Zhou. THE PLASTIC DEFORMATION AND EFFECT OF HYDROGEN ON DEFORMATION OF Ni-P AMORPHOUS COATINGS. Acta Metall Sin, 2007, 42(1): 87-90 .

Download:  PDF(259KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The plastic deformation and effect of hydrogrn on deformation of electroless Ni-P amorphous coatings were studied through indentation test. The results showed that circular shear bands formed around the indent and the plastic zone size increased linearly with the square root of the applied load, hydrogen could enhance localized plastic deformation, deduced the yield strength.
Key words:  Ni-P coating      hydrogen      indentation      plastic deformation      
Received:  18 May 2006     
ZTFLH:  TG113  

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V42/I1/87

[1] Kramer D,Huang H,Kriese M,Robach J,Nelson J, Wright A,Bahr D,Gerberich W W.Acta Mater,1999; 47:333
[2] Vaidyanathan R,Dao M,Ravichandran G,Suresh S. Acta Mater, 2001; 49:3781
[3] Schuh C A,Nieh T G.Acta Mater,2003;5l:87
[4] Jana S,Bhowmick R,Kawamura Y,Chattopadhyay K, Ramamurty U.Intermetallics,2004; 12:1097
[5] Jana S,Ramamurty U,Chattopadhyay K,Kawamura Y. Mater Sci Eng, 2004; A375—377:1191
[6] Greer A L,Castellero A,Madge S V,Walker I T,Wilde J R.Mater Sci Eng, 2004; A375-377:1182
[7] Ramamurty U, Jana S,Kawamura Y,Chattopadhyay K.Acta Mater,2005;53:705
[8] Wu X F,Zhang H F,Li H,Wang A M,Yang H C,Hu Z Q.Chin J Nonferrous Met,2003;13:1368) (武晓峰,张海峰,李宏,王爱民,杨洪才,胡壮麒.中国有色金属学报,2003;13:1368)
[9] Lin J J,Perng T P.Metall Mater Trans,1995;26A:197
[10] Namboodhiri T K,Ramesh T A,Singh G,Seghal S. Mater Sci Eng, 1983; 61:23
[11] Suh D,Dauskardt R H.Scr Mater,2000;42:233
[12] Wang Y W,Chu W Y,Li J X,Hui X D,Wang Y B,Gao K W,Qiao L J.Mater Lett,2004; 58:2393
[13] Reidel W.Electroless Nickel Plating.London:Finishing Publications, 1991:1
[14] Zhou Q J,He J Y,Li J X,Chu W Y,Qiao L J.Mater Lett,2006;60:349
[15] Peng X,Su Y J,Gao K W,Qiao L J,Chu W Y.Mater Lett,2004;58:2073
[16] dos Santos D S,de Biasi R S,de Miranda P E V.J Non Cryst Solids, 1997;210:136
[17] Johnson K L.J Mech Phys Solids,1970;18:115
[18] Tao S J.J Chem Phys,1972;56:5499
[19] Eldrup M,Colemal P G.Positron Annihilation.Amster- dam:North—Holland, 1982:1
[20] Hagiwara K,Ougizawa T,Inoue T,Hirata K,Kobayashi Y.Radiat Phys Chem, 2000;58:525T
[1] ZHANG Haifeng, YAN Haile, FANG Feng, JIA Nan. Molecular Dynamic Simulations of Deformation Mechanisms for FeMnCoCrNi High-Entropy Alloy Bicrystal Micropillars[J]. 金属学报, 2023, 59(8): 1051-1064.
[2] WAN Tao, CHENG Zhao, LU Lei. Effect of Component Proportion on Mechanical Behaviors of Laminated Nanotwinned Cu[J]. 金属学报, 2023, 59(4): 567-576.
[3] LI Qian, SUN Xuan, LUO Qun, LIU Bin, WU Chengzhang, PAN Fusheng. Regulation of Hydrogen Storage Phase and Its Interface in Magnesium-Based Materials for Hydrogen Storage Performance[J]. 金属学报, 2023, 59(3): 349-370.
[4] DU Zonggang, XU Tao, LI Ning, LI Wensheng, XING Gang, JU Lu, ZHAO Lihua, WU Hua, TIAN Yucheng. Preparation of Ni-Ir/Al2O3 Catalyst and Its Application for Hydrogen Generation from Hydrous Hydrazine[J]. 金属学报, 2023, 59(10): 1335-1345.
[5] DING Zongye, HU Qiaodan, LU Wenquan, LI Jianguo. In Situ Study on the Nucleation, Growth Evolution, and Motion Behavior of Hydrogen Bubbles at the Liquid/ Solid Bimetal Interface by Using Synchrotron Radiation X-Ray Imaging Technology[J]. 金属学报, 2022, 58(4): 567-580.
[6] GUO Xiangru, SHEN Junjie. Modelling of the Plastic Behavior of Cu Crystal with Twinning-Induced Softening and Strengthening Effects[J]. 金属学报, 2022, 58(3): 375-384.
[7] REN Shaofei, ZHANG Jianyang, ZHANG Xinfang, SUN Mingyue, XU Bin, CUI Chuanyong. Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism[J]. 金属学报, 2022, 58(2): 129-140.
[8] ZHU Bin, YANG Lan, LIU Yong, ZHANG Yisheng. Micromechanical Properties of Duplex Microstructure of Martensite/Bainite in Hot Stamping via the Reverse Algorithms in Instrumented Sharp Indentation[J]. 金属学报, 2022, 58(2): 155-164.
[9] XIAO Na, HUI Weijun, ZHANG Yongjian, ZHAO Xiaoli. Hydrogen Embrittlement Behavior of a Vacuum-Carburized Gear Steel[J]. 金属学报, 2021, 57(8): 977-988.
[10] AN Xudong, ZHU Te, WANG Qianqian, SONG Yamin, LIU Jinyang, ZHANG Peng, ZHANG Zhaokuan, WAN Mingpan, CAO Xingzhong. Interaction Mechanism of Dislocation and Hydrogen in Austenitic 316 Stainless Steel[J]. 金属学报, 2021, 57(7): 913-920.
[11] LAN Liangyun, KONG Xiangwei, QIU Chunlin, DU Linxiu. A Review of Recent Advance on Hydrogen Embrittlement Phenomenon Based on Multiscale Mechanical Experiments[J]. 金属学报, 2021, 57(7): 845-859.
[12] SUN Xiaojun, HE Jie, CHEN Bin, ZHAO Jiuzhou, JIANG Hongxiang, ZHANG Lili, HAO Hongri. Effect of Fe Content on the Microstructure, Electrical Resistivity, and Nanoindentation Behavior of Zr60Cu40-xFex Phase-Separated Metallic Glasses[J]. 金属学报, 2021, 57(5): 675-683.
[13] SHI Zengmin, LIANG Jingyu, LI Jian, WANG Maoqiu, FANG Zifan. In Situ Analysis of Plastic Deformation of Lath Martensite During Tensile Process[J]. 金属学报, 2021, 57(5): 595-604.
[14] LIN Pengcheng, PANG Yuhua, SUN Qi, WANG Hangduo, LIU Dong, ZHANG Zhe. 3D-SPD Rolling Method of 45 Steel Ultrafine Grained Bar with Bulk Size[J]. 金属学报, 2021, 57(5): 605-612.
[15] CAO Qingping, LV Linbo, WANG Xiaodong, JIANG Jianzhong. Magnetron Sputtering Metal Glass Film Preparation and the “Specimen Size Effect” of the Mechanical Property[J]. 金属学报, 2021, 57(4): 473-490.
No Suggested Reading articles found!