| The influence of strain rate and temperature on flow stress and critical dynamic recrystallisation of T122 steel |
| Cao Jin-Rong;;; |
|
Cite this article:
Cao Jin-Rong. The influence of strain rate and temperature on flow stress and critical dynamic recrystallisation of T122 steel. Acta Metall Sin, 2007, 42(1): 35-40 .
|
|
|
Abstract The hot deformation behavior of the heat resistant steel T122 was investigated
with a compression test on Gleeble 3500 simulator at a temperature range of
900--1200 ℃ and strain rate range of 10 -2—10 1 s -1.
A method was developed to determine the
activation energy and material parameters
in the hyperbolic sine constitutive equation. The
activation energies determined are 570 kJ/mol and
548 kJ/mol for steel T122 in saturation stress
and peak stress, respectively. The values of
critical strain for dynamic recrystallization
(DRX) initiation was determined from
the strain-stress curves, a equation related to the
Zener-Hollomon parameter was obtained.
|
|
Received: 08 June 2006
|
|
|
[1] Fujimitu M.ISIJ Int,2001;41:612 [2] Niu J T.Physical Simulation Technology of Materials During Hot Processing.Beijing:National Defence Press, 1999:149 (牛济泰.材料和热加工领域的物理模拟技术.北京:国防工业出版社,1999:149) [3] Davenport S B,Silk N J,Sellars C M.Mater Sci Teehnol, 2000;16:539 [4] Sellars C M.In:Krausz G,ed.,Deformation Processing and Structure,Metals Park,0H:ASM,1983:245 [5] McQueen H J,Yue S,Ryan N D,Fry E.J Mater Process Technol,1995;53:293 [6] McQueen H J,Yue S,Ryan N D.Mater Sci Eng,2002; A322:43 [7] Medina S F,Hernandez C A.Acta Mater,1996;44:137 [8] Carsl M,Allende R,Penalba F,Jimenez J A,Ruano O A.Steel Res Int,2004;75(1):26 [9] Zhu F X,Liu C,Wang P,Gao D F,Gao C,Zhu C Q,Ni G Z.Steel Pipe,1999;28(1):8 (朱伏先,刘川,王平,高德福,高潮,祝春清,倪国政.钢管,1999;28(1):8) [10] Penalba F,Carsl M,Larrea M T,Ruano O A,Allende R.In:14th Rolling Conf, San Nicolas,Buenos Aires,Ar- gentina:Instituto Argentino de Siderurgia,2002:383 [11] Imbert C,Ryan N D,McQueen H J.Metall Trans,1984; 15A:1855 [12] Poliak E I,Jonas J J.Acta Mater,1996;44:127 [13] Zahiri S D,Davies C H G,Hodgson P D.Scr Mater,2005; 52:299 [14] Imbert C A C,McQueen H J.Mater Sci Eng,2001;A313: 104 |