Please wait a minute...
Acta Metall Sin  2007, Vol. 42 Issue (1): 27-34     DOI:
Research Articles Current Issue | Archive | Adv Search |
Microstructure Evolution of medium carbon steel during deformation of undercooled austenite
;
北京科技大学
Cite this article: 

;. Microstructure Evolution of medium carbon steel during deformation of undercooled austenite. Acta Metall Sin, 2007, 42(1): 27-34 .

Download:  PDF(1161KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  The microstructure evolution of a medium carbon steel (0.48%C) during deformation of undercooled austenite at different deformation temperature and strain rate has been investigated by means of uniaxial hot compression simulation experiment. The predominant mechanism on the formation of ultrafine (冄+冡) microduplex structures has been studied in medium carbon steel The experimental results showed that the process of microstructure development can be divided into three stages: dynamic ferrite transformation, dynamic pearlite transformation and spheroidization of lamellae pearlite. And the effects of deformation temperature and strain rate on the process of dynamic transformation and spheroidization of pearlite were different. A large number of vacanies and high density dislocations introduced during large strain hot deformation provided short-circuiting paths for diffusion of carbon atoms, as a result the rate of cementite spheroidization was accelerated by four orders of magnitude through deformation of undercooled austenite as compared to a static annealing treatment. The redistribution of cementite particles in the ferrite matrix has been observerd, which can be interpreted in terms of dissolution-reprecipitation mechanism.
Key words:  medium carbon steel      dynamic transformation      spheroidization of pearlite      diffusion of carbon atoms      
Received:  17 April 2006     
ZTFLH:  TG111.2 TG142.31  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2007/V42/I1/27

[1] Shin D H,Kim B C,Park K T,Kim Y S.Acta Mater, 2000;48:2247
[2] Ivanisenko Y,Lojkowski W,Valiev R Z,Fecht H J.Acta Mater,2003;51:5555
[3] Yang W Y,Hu A M,Qi J J,Sun Z Q.Chin J Mater Res, 2001:15:17l (杨王玥,胡安民,齐俊杰,孙祖庆.材科研究学报,200l;15: 171)
[4] Beladi H,Kelly G L,Shokouhi A,Hodgson P D. Mater Sci Eng,2004;A367:152
[5] Choi J K,Seo D H,Lee J S,Um K K,Choo W Y. ISIJ Int,2003;43:746
[6] Ashby M F.Philos Mag,1966;14:l157
[7] Furuhara T,Mizoguchi T,Maki T.ISIJ Int,2005;45:392
[8] Storojeva L,Ponge D,Kaspar R,Raabe D.Acta Mater, 2004; 52:2209
[9] Hillert M.In:Zackay V F, Aaronson H I,eds.,Decompo- sition of Austenite by Diffusional Processes,New York: Interscience, 1962:198
[10] Robbins J L,Shepard O C,Sherby O D.J Iron Steel Inst, 1964;202:804
[11] Wert C A.Phys Rev, 1950; 79:60l
[12] Chattopadhyay S, Sellars C M.Acta Metall, 1982;30:l57
[13] Harrigan M J, Sherby O D.Mater Sci Eng,1971; 7:177
[14] Hono K, Ohnuma M,Murayama M,Nishida S,Yoshie A, Takahashi T.Scr Mater,2001; 44:977
[15] Gavriljuk V G.Mater Sci Eng, 2003;A345:8l
[16] Shin D H, Kim B C, Kim Y S.Scr Mater,2003;48:469
[1] Huidong WU, Goro MIYAMOTO, Zhigang YANG, Chi ZHANG, Hao CHEN, Tadashi FURUHARA. Incomplete Bainite Transformation Accompanied with Cementite Precipitation in Fe-1.5(3.0)%Si-0.4%C Alloys[J]. 金属学报, 2018, 54(3): 367-376.
[2] WU Si, LI Xiucheng, ZHANG Juan, SHANG Chengjia. EFFECT OF Nb ON TRANSFORMATION AND MICROSTRUCTURE REFINEMENT IN MEDIUM CARBON STEEL[J]. 金属学报, 2014, 50(4): 400-408.
[3] WANG Bin, LIU Zhenyu, ZHOU Xiaoguang, WANG Guodong. EFFECT OF COOLING PATH ON THE HOLE-EXPANSION PROPERTY OF MEDIUM CARBON STEEL[J]. 金属学报, 2012, 48(4): 435-440.
[4] YIN Yunyang YANG Wangyue LI Longfei SUN Zuqing WANG Xitao . MICROSTRUCTURE CONTROL OF HOT ROLLED TRIP STEEL BASED ON DYNAMIC TRANSFORMATION OF UNDERCOOLED AUSTENITE
II. Cooling Rate After Dynamic Transformation of Undercooled Austenite
[J]. 金属学报, 2010, 46(2): 161-166.
[5] ZHANG Han BAI Bingzhe. MICROSTRUCTURAL\, EVOLUTION OF Mn-Si-Cr MEDIUM CARBON STEEL DEFORMED UNDER UNDERCOOLED AUSTENITE STATE[J]. 金属学报, 2010, 46(1): 47-51.
[6] ZHANG Jiwang LU Liantao ZHANG Weihua. ANALYSIS ON FATIGUE PROPERTY OF MICROSHOT PEENED MEDIUM CARBON STEEL[J]. 金属学报, 2009, 45(11): 1378-1383.
[7] . Study on Microstructure Evaluation of hot rolled C-Mn-Si-Al TRIP steel based on dynamic transformation of undercooled austentie[J]. 金属学报, 2008, 44(6): 686-692 .
[8] LI Longfei. INFLUENCE OF THE PARTIAL SUBSTITUTION OF SI BY AL ON THE MICROSTRUCTURE OF THE HOT ROLLING TRIP STEELS BASED ON DYNAMIC TRANSFORMATION OF UNDERCOOLED AUSTENITE[J]. 金属学报, 2008, 44(11): 1292-1298 .
[9] LI Longfei. STUDY ON MICROSTRUCTURE AND MECHANICAL PROPERTIES OF HOT ROLLIED C-Mn-Si-(Al) TRIP STEELS BASED ON DYNAMIC TRANSFORMATION OF UNDERCOOLED AUSTENITE[J]. 金属学报, 2008, 44(11): 1299-1304 .
[10] . The distribution and diffusion of carbon atoms during deformation of undercooled austenite in medium carbon steel[J]. 金属学报, 2007, 43(8): 785-790 .
[11] HUI Weijun; TIAN Peng; DONG Han; SU Shihuai; YU Tongren; WENG Yuqing. Influence of Deformation Temperature on the Microstructure Transformation in Medium Carbon Steel[J]. 金属学报, 2005, 41(6): 611-616 .
[12] LIU Yumen;HE Zhirong Xi'an Jiaotong University. SOME CHARCTERISTICS OF MARTENSITE IN MEDIUM CARBON IRON ALLOY[J]. 金属学报, 1989, 25(2): 61-64.
No Suggested Reading articles found!