Abstract Solute diffusion controlled solidification model were applied to simulate the initial stage cellular to dendrite transition of Ti55Al45 alloys during directional solidification at different velocities. The simulation results show,during cellular/dendritic transition , mixed structure zone composed of cells and dendrites was observed ,with two parallel closely spaced dendrites with secondary dendrites absent at the facing surfaces . The dendrite spacing are larger than that of cellular spacing at a given rate, the columnar grain spacing sharply increases to a maximum as solidification advance to coexistence zone. In addition, simulation also revealed the numbers of the seeds also exert an influence on the grain spacing, with increasing the numbers of the seed, the uniform degree of the columnar grain spacing tends to increase. Lastly the main influence factors of affecting cellular/dendritic transition were analyzed, which could be dendrite growth resulting in slight fluctuations of liquid composition occurred at growth front. The simulation results also are in reasonable agreement with experiment observation at low cooling rates.
|
|
Received: 08 May 2006
|
|
|
[1]Lan C W,Chang Y C.J Cryst Growth,2003;250:525 [2]Warren J A,Langer J S.Phys Rev,1990;42A:3518 [3]Kurz W,Fisher J D.Acta Metall,1981;29:12 [4]Lapin J,OndrúL,Nazmy M.Intermetallics,2002;10:1019 [5]Warren J A,Langer J S.Phys Rev,1993;47E:2702 [6]Rappaz M,Gandin C A.Acta Metall Mater,1993;41:345 [7]Nastac L,Stefanescu D M.Mater Sci Eng,1997;54:391 [8]Nastac L.Acta Mater,1999;17:4253 [9]Xu Q Y,Liu B C.J Mech Eng,2001;12:328(许庆彦,柳百成.中国机械工程,2001;12:328) [10]Zhu M F,Chen J,Sun G X,Hong C P.Acta Metall Sin,2005:41:583(朱鸣芳,陈晋,孙国雄,洪俊杓.金属学报,2005;41:583) [11]Li Q,Li D Z,Qian B N.Acta Metall Sin,2004;40:634(李强,李殿中,钱百年.金属学报,2004;40:634) [12]Su Y Q,Liu C,Li X Z,Guo J J,Li B S,Jia J,Fu H Z.Intermetallics,2005;13:270 [13]Wagner A,Shollock B A,McLean M.Mater Sci Eng,2004;A374:270 [14]Mathiesen R H,Arnberg L.Acta Mater,2005;53:950 [15]Johnson D R,Chihara K,Inui H,Yamguch M M.Acta Mater,1998;18:6537 [16]Hunt J D,Lu S Z.Metall Mater Trans,1996;27A:611 [17]Mullins C W,Sekerka R F.J Appl Phys,1964;35:444 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|