Cite this article:
. . Acta Metall Sin, 2007, 43(6): 595-598 .
|
|
|
Abstract ABSTRACT Superfine Ti-O inclusions are of great importance for the quality of steel.This work adopts directional solidification method to simulate the precipitation of inclusions because of solute enrichment between secondary dendrite, thereby investigates the effect of cooling rate on the size and number of Ti—O inclusions, furthermore verifies a coupled model of microsegregation and Ti-O inclusion precipitation during solidification of liquid steel. The experimental results indicate that the inclusion size is minished, the number is increased and the distribution is more symmetrical when enhancing cooling rates.The average diameters of inclusions are 1.86μm,1.17μm and 0.84μm,the numbers per unit volume are 0.31×104mm-3,1.98×104mm-3 and 3.27×104mm-3 when the cooling rates are 10k/min,100k/min and 200k/min,furthermore it has been proved that superfine inclusions precipitated during solidification is feasible.
|
|
Received: 11 September 2006
|
|
|
[1]Hedjazi D,Bennett F H J,Kondic V.Br Foundryman, 1975;68:305 [2]Zhang D T.The Identification of Non-Metal Inc lusions in Steel Beijing:National Defence Industry Press,1991 (张德堂.钢中非金属夹杂物鉴别.北京,国防工业出版社,1991) [3]Li D Z.Non-Metal Inclusions in Steel.Beijing:Science Press,1983 (李代锤.钢中的非金属夹杂物.北京:科学出版社,1983) [4]Mizoguchi S,Takamura J.Proc 6th Iron and Steel Congress,Vol.1,Tokyo:ISIJ,1990:598 [5]Sawai T,Wakoh M,Ueshima Y,Mizoguchi S.Proc 6th Iron and Steel Cong,Vol.1,Tokyo:ISIJ,1990:605 [6]Ogibayashi S,Yamaguchi K,Hirai M,Goto H,Yamaguchi H,Tanaka K.Proc 6th Iron and Steel Congress,Vol.1, Tokyo:ISIJ,1990:612 [7]Babu S S,David S A,Vitek J M,Mundra K,Debroy T. Mater Sci Technol,1995;11:187 [8]Takamura J,Mizoguchi S.Proc 6th Iron and Steel Cong, Vol.1,Tokyo:ISIJ,1990:591 [9]Liu Z Z,Wei J,Cai K K.ISIJ Int,2002;42:958 [10]Suzuki M,Yamaguchi R,Murakami K,Nakada M.ISIJ Int,2001;41:247 [11]Ovtchinnikov S,Kazakov S,Janke D.Ironmaking Steel- making,2003;30:487 [12]Wintz M,Bobadilla M,Lehmann J,Gaye H.ISIJ Int, 1995;35:715 [13]Ma Z T,Janke D.ISIJ Int,1998;38:46 [14]Zhang H Q,Zheng S B,Zheng Q,Liu Z L,Jiang G C. Acta Metall Sin,2006;42:745 (张会全,郑少波,郑庆,刘自立,蒋国昌.金属学报,2006; 42:745) [15]Final Report of Fine Inclusions Committee.Tokyo:The Iron and Steel Institute of Japan,1995:116 [16]Byun J S,Shim J H,Cho Y W,Lee D N.Acta Mater, 2003;51:1593 [17]Z G Yang.Heat Treat Met,2005;30(1):20 [18]Zhang H Q.Master Thesis,Shanghai University,2006 (张会全.上海大学硕士学位论文,2006) |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|