Abstract Among all the processing parameters which affect porous structure obtained by directional solidification of a solid/gas (e.g. metal/hydrogen) eutectic (Gasar), the gas pressure above melts and the superheating temperature of melts are the most observable and easily governed because they directly control the amount of hydrogen saturated in melts. The critical processing conditions for hydrogen to escape and for formation of lotus-type porous structure have been deduced through theoretical analysis and calculation, and the following conclusions have been obtained: both the superheating temperature and the argon partial pressure should have moderate values, viz. with given partial pressures of hydrogen and argon, the superheating temperature should be bigger than the threshold of formation of lotus-type structure and smaller than that of hydrogen to escape; however, with given superheat degree and hydrogen partial pressure, the argon partial pressure should be bigger than the threshold of hydrogen to escape and smaller than that of formation of lotus-type porous structure. These conclusions were verified by the experimental results of lotus-type porous Mg and will contribute to the fabrication of high-quality regular porous metals by Gasar process.
[1]Shapovalov V I.U S Pat,5,181,549,1993 [2]Liu Y,Li Y X,Wan J,Zhang H W.Mater Sci Eng,2005; A402:47 [3]Zhang H W,Li Y X,Liu Y.Acta Metall Sin,2006;42: 1165 (张华伟,李言样,刘源.金属学报,2006;42:1165) [4]Liu Y,Li Y X,Zhang H W,Wan J.Acta Metall Sin,2005; 41:886 (刘源,李言祥,张华伟,万疆.金属学报,2005;41:886) [5]Liu Y,Li Y X,Zhang H W,Wan J.J Mater Sci Technol, 2006;22:306 [6]Li Y X,Liu Y,Zhang H W,Wang X.In:Nakajima H, Kanetake N eds.,Proc MetFoam 2005,Sendai:The Japan Institute of Metals,2006:237 [7]Zhu M Y,Xiao Z Q.Mathematical and Physical Simu- lation of Steel Refining Process.Beijing:Metallurgical Industry Press,1998:1 (朱苗勇,萧泽强.钢的精炼过程数学物理模拟.北京:冶金工业出版社,1998:1) [8]Han Q Y.Kinetics on Metallurgical Process.Beijing: Metallurgical Industry Press,1983:167 (韩其勇.冶金过程动力学.北京:冶金工业出版社,1983:167) [9]Smithells C J.Smithells Metals Reference Book.7th ed., Boston:Butterworth-Heinemann,1992:14-7 [10]Miedema A R,Boom R.Z Metallkd,1978;69:183 [11]Shapovalov V I,Semik A P,Timchenko A G.Metallurgy, 1993;3:25 [12]Yamamura S,Shiota H,Murakami K.Mater Sci Eng, 2001;A318:137 [13]An G Y.Formation Theory of Castings.Beijing:China Machine Press,1989:173 (安阁英.铸件形成理论.北京:机械工业出版社,1989:173) [14]Apprill J M,Poirier D R,Maguire M C,Gutsch T C. Mater Res Soc Symp Proc,1998;521:291