Please wait a minute...
Acta Metall Sin  2008, Vol. 44 Issue (1): 1-7     DOI:
Research Articles Current Issue | Archive | Adv Search |
SUPERPLASTICITY OF ALUMINIUM SERIES INTERMETALLIC COMPOUND
;;
吉林大学超塑性与塑性研究所
Cite this article: 

. SUPERPLASTICITY OF ALUMINIUM SERIES INTERMETALLIC COMPOUND. Acta Metall Sin, 2008, 44(1): 1-7 .

Download:  PDF(366KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on basic conceptions of superplasticity and intermetallic compound, the significance of studying the supeplasticity of intermetallic compound is adressed. And recent advances in superplasticity in Ni-Al, Ti-Al and Fe-Al aluminium series intermetallic componund are reviewd.
Key words:  structural material      aluminium series intermetallic compound      superplasticity      
Received:  15 August 2007     
ZTFLH:  TG146.2  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2008/V44/I1/1

[1]Wu S D.Theory of Metal Superplastic Deformation.Bei- jing:National Defence Industry Press,1997:1 (吴诗惇.金属超塑性变形理论.北京:国防工业出版社,1997:1)
[2]Chokshi A H,Mukherjee A K,Langdon T G.Mater Sci Eng,1993;R10:237
[3]Song Y Q.Aeronaut Manuf Technol,2003;(7):17 (宋玉泉.航空制造技术,2003;(7):17)
[4]Chen G L.Shanghai Met,2002;24(4):1 (陈国良.上海金属,2002;24(4):1)
[5]Fan R H,Bian X F,Yin Y S.Shandong Sci,1997;10(1): 6 (范润华,边秀房,尹衍升.山东科学,1997;10(1):6)
[6]Zhang L T,Mao DL,Wu J S.Shanghai Met,1999;21(2): 18 (张澜庭,毛大立,吴建生.上海金属,1999;21(2):18)
[7]Nieh T G,Wadsworth J.Acta Metall Sin(Engl Lett), 1995;8(Z1):405
[8]Liu C T,White C L,Horton J A.Acta Metall,1985;33: 213
[9]Wright R N,Sikka V K.J Mater Sci,1988;23:4315
[10]Mukhopadhyay J,Kaschner G,Mukherjee A K.Scr Met- all Mater,1990;24:857
[11]Valiev R Z,Gayanov R M,Yang H S,Mukherjee A K.Scr Metall Mater,1991;25:1945
[12]Guo J T.Ordered Intermetallic Compound NiAl Alloy. Beijing:Science Press,2003:231 (郭建亭.有序金属间化合物镍铝合金.北京:科学出版社,2003:231)
[13]Mishra R S,Valiev R Z,McFadden S X,Mukherjee A K. Mater Sci Eng,1998;A252:174
[14]McFadden S X,Valiev R Z,Mukherjee A K.Mater Sci Eng,2001;A319-321:849
[15]Gu Y F,Lin D L,Shan A D,Liu Y,Liu Z Y.Acta Metall Sin,1997;33:325 (谷月峰,林栋梁,单爱党,刘毅,刘震云.金属学报,1997;33:325)
[16]Guha S,Baker I,Munroe P R.J Mater Sci,1996;31: 4055
[17]Chen R S,Guo J T,Yin W M,Zhou J Y.Acta Metall Sin,1998;34:1121 (陈荣石,郭建亭,殷为民,周继扬.金属学报,1998;34:1121)
[18]Chen R S,Guo J T,Yin W M,Zhou J Y.Scr Mater,1999; 40:209
[19]Zhou W L,Guo J T,Chen R S,Zhou J Y.Acta Metall Sin,1999;35:995 (周文龙,郭建亭,陈荣石,周继扬.金属学报,1999;35:995)
[20]Zhou W L,Guo J T,Chen R S,Li G S,Zhou J Y.Mater Lett,2001;47:30
[21]Zhou W L,Guo J T,Chen R S,Zhou J Y.Acta Metall Sin,2000;36:796 (周文龙,郭建亭,陈荣石,周继扬.金属学报,2000;36:796)
[22]Zhou W L,Guo J T,Chen R S,Zhou J Y.Mater Lett, 2001;51:342
[23]Du X H,Guo J T,Zhou B D.Acta Metall Sin,2001;37: 1112 (杜兴蒿,郭建亭,周彼德.金属学报,2001;37:1112)
[24]Du X H,Guo J T,Zhou B D.Mater Lett,2002;52:442
[25]Sundar R S,Kitazono K,Sato E,Kuribayashi K.Acta Mater,2001;49:1717
[26]Du X H,Guo J T,Zhou B D.Scr Mater,2001;45:69
[27]Du X H,Guo J T,Zhou B D.Acta Metall Sin,2001;37: 144 (杜兴蒿,郭建亭,周彼德.金属学报,2001;37:144)
[28]Du X H,Guo J T,Zhou B D,Xiong L Y.J Mater Sci Technol,2003;19:373
[29]Hu J,Lin D L.Mater Lett,2004;58:1297
[30]Jiang D M,Lin D L.Mater Lett,2002;57:747
[31]Jiang D M,Lin D L.J Shanghai Jiaotong Univ,2002;36: 597 (蒋冬梅,林栋梁.上海交通大学学报,2002;36:597)
[32]Qi Y H,Guo J T,Cui C Y,Li G S.Mater Lett,2002;57: 552
[33]Cui C Y,Guo J T,Qi Y H,Ye H Q.Acta Metall Sin, 2002;38:679 (崔传勇,郭建亭,齐义辉,叶恒强.金属学报,2002;38:679)
[34]Qi Y H,Guo J T,Cui C Y.Chin J Nonferrous Met,2002; 12:245 (齐义辉,郭建亭,崔传勇,中国有色金属学报,2002;12:245)
[35]Zhang J M,Li S Q,Zou D X,Zhong Z Y.J Iron Steel Res,1995;7(6):75 (张建民,李世琼,邹敦叙,仲增墉.钢铁研究学报,1995;7(6):75)
[36]Ameyama K,Fujii T,Okumura T,Sodeoka S,Tokizane M.Mater Sci Forum,1997;233-234:287
[37]Bohn R,Klassen T,Bormann,R.Intermetallics,2001;9: 559
[38]Lu S Q,Huang B Y,He Y H.J Nanchang Inst Aeronaut Technol(Nat Sci),2001;15(4):6 (鲁世强,黄伯云,贺跃辉.南昌航空工业学院学报(自然科学版),2001;15(4):6)
[39]Sun J,Wu J S,Zhang H Y,He Y H,Deng Z Y.Rare Met Mater Eng,2000;29:13 (孙坚,吴建生,张惠义,贺跃辉,邓忠勇.稀有金属材料与工程,2000;29:13)
[40]Huang B Y,He Y H,Deng Z Y,Wang J N,Sun J.Acta Metall Sin,1998;34:1173 (黄伯云,贺跃辉,邓忠勇,王健农,孙坚.金属学报,1998;34:1173)
[41]Sun F,Lin D L.J Shanghai Jiaotong Univ,2001;35:380 (孙锋,林栋梁.上海交通大学学报,2001;35:380)
[42]Deng Z Y,Huang B Y,He Y H,Liu Y.J Mater Eng,1999; (12):26 (邓忠勇,黄伯云,贺跃辉,刘咏.材料工程,1999;(12):26)
[43]Mishra R S,Mukherjee A K.d Mater Sci,2000;35:147
[44]Imayev R M,Kaibyshev O A,Salishchev G A.Acta Metall Mater,1992;40:581
[45]Imayev V M,Imayev R M,Kuznetsov A V,Shagiev M R, Salishchev G A.Mater Sci Eng,2003;A348:15
[46]Zhou K C,Huang B Y,Qu X H.J Central South Univ Technol,1998;29:559 (周科朝,黄伯云,曲选辉.中南工业大学学报,1998;29:559
[47]Zhou K C,Huang B Y,Qu X H,Chen X Q.Rare Met Mater Eng,1998;27:336 (周科朝,黄伯云,曲选辉,陈小群.稀有金属材料与工程,1998;27:336)
[48]Zhou K C,Huang B Y,Qu X H.Chin J Rare Met,1999; 23:394 (周科朝,黄伯云,曲选辉.稀有金属,1999;23:394)
[49]Sun J,Liu R K,Wu J S,He Y H.Acta Metall Sin,2001; 37:95 (孙坚,刘润开,吴建生,贺跃辉.金属学报,2001;37:95)
[50]Sun J,Fu Y F,Wu J S,He Y H.J Mater Eng,1999;(9): 13 (孙坚,傅拥峰,吴建生,贺跃辉.材料工程,1999;(9):13)
[51]Shi X H,Zhang D,Ge Y,Qin J N,Zhang G D.Mater Sci Eng,1998;16:24 (施幸华,张荻,葛云,覃继宁,张国定.材料科学与工程,1998;16:24)
[52]Zhang D,Qin J N,Shi X H.Rare Met Mater Eng,1998; 27:210 (张荻,覃继宁,施幸华.稀有金属材料与工程,1998;27:210)
[53]Sun F,Lin D Y.Trans Nonferrous Met Soc Chin,2002; 12:615
[54]Durra A,Banerjee D.Scr Metall Mater,1990;24:1319
[55]Yang H S,]in P,Mukherjee A K.Mater Sci Eng,1992; A153:457
[56]Wang B,Jia T C,Zou D X,Mall P,Zhong Z Y.Mater Sci Eng,1992;A153:422
[57]Wang B,Jia T C,Wang Y Q,Zou D X,Zhong Z Y.Acta Metall Sin,1994;30:B309 (王斌,贾天聪,王跃群,邹敦叙,仲增墉.金属学报,1994;30:B309)
[58]Song D,Ding H,Wang D L.J Northeastern Univ(Nat Sci),2001;22:660 (宋丹,丁桦,王殿梁.东北大学学报(自然科学版),2001;22:660)
[59]Ding H,Song D,Du Y H,Zhang C B,Cui J Z,Bai B Z, Wan C J.J Iron Steel Res,1999;11(3):34 (丁桦,宋丹,杜云蕙,张彩碚,崔建忠,白秉哲,万初杰.钢铁研究学报,1999;11(3):34)
[60]Sun F S,Ma J M,Cao C X.Acta Metall Sin,1994;30: B465 (孙福生,马济民,曹春晓.金属学报,1994;30:B465)
[61]Imayev R M,Gabdullin N,Salishchev G.Intermetallics, 1997;5:229
[62]Rosenberg Y,Mukherjee A K.Mater Sci Eng,1995; A192/193:788
[63]Li D Q,Liu Y,Shan A D,Lin D L.Acta Metall Sin,1996; 32:417 (郦定强,刘毅,单爱党,林陈梁.金属学报,1996;32:417)
[64]Li D Q,Shan A D,Liu Y,Lin D L.Scr Metall Mater, 1995;33:681
[65]Liu Y,Li D Q,Lin D L,Chen S P,Zhao X N,Hong J M. J Chin Electron Microsc Soc,1995;14:421 (刘毅,郦定强,林栋梁,陈世仆,赵晓宁,洪建明.电子显微学报,1995;14:421)
[66]Li D Q,Lin D L,Liu J L,Liu Y.Acta Metall Sin,1997; 33:897 (郦定强,林栋梁,刘俊亮,刘毅.金属学报,1997;33:897)
[67]Lin D,Li D,Liu Y.Intermetallics,1998;6:243
[68]Lin D,Liu Y.Mater Sci Eng,1999;A268:83
[69]Lin D,Shan A,Li D.Scr Metall Mater,1994;31:1455
[70]Lin D,Lin T L,Shan A,Chen M.Intermetallics,1996;4: 489
[71]Hu J,Lin D L.Trans Mater Heat Treat,2003;24:31 (胡静,林栋梁.材料热处理学报,2003;24:31)
[72]Chen M W,Shan A D,Lin D L.Trans Met Heat Treat, 1995;16(3):9 (陈明伟,单爱党,林栋梁.金属热处理学报,1995;16(3):9)
[73]Yang Y J,Shan A D,Lin D L.J Shanghai College Metall, 1999;20(3):140 (羊忆军,单爱党,林栋梁.上海冶金高等专科学校学报,1999;20(3):140)
[74]Gao D C,Yang W Y,Huang X X,Sun Z Q.Acta Metall Sin,2001;37:291 (高德春,杨王玥,黄晓旭,孙祖庆.金属学报,2001;37:291)
[75]Sharma G,Kishore R,Sundararaman M,Ramanujan R V.Mater Sci Eng,2006;A419:144
[76]Guo J T,Zhou W L.Mater Rev,2000;14(5):18 (郭建亭,周文龙.材料导报,2000;14(5):18)
[1] WANG Huiyuan, XIA Nan, BU Ruyu, WANG Cheng, ZHA Min, YANG Zhizheng. Current Research and Future Prospect on Low-Alloyed High-Performance Wrought Magnesium Alloys[J]. 金属学报, 2021, 57(11): 1429-1437.
[2] Guangming XIE, Zongyi MA, Peng XUE, Zongan LUO, Guodong WANG. Effects of Tool Rotation Rates on Superplastic Deformation Behavior of Friction Stir Processed Mg-Zn-Y-Zr Alloy[J]. 金属学报, 2018, 54(12): 1745-1755.
[3] Huiyuan WANG, Hang ZHANG, Xinyu XU, Min ZHA, Cheng WANG, Pinkui MA, Zhiping GUAN. Current Research and Future Prospect on Microstructure Stability of Superplastic Light Alloys[J]. 金属学报, 2018, 54(11): 1618-1624.
[4] ZHANG Xinming, DENG Yunlai, ZHANG Yong. DEVELOPMENT OF HIGH STRENGTH ALUMINUM ALLOYS AND PROCESSING TECHNIQUES FOR THE MATERIALS[J]. 金属学报, 2015, 51(3): 257-271.
[5] Chao YANG,Jijie WANG,Zongyi MA,Dingrui NI,Mingjie FU,Xiaohua LI,Yuansong ZENG. FRICTION STIR WELDING AND LOW-TEMPERATURE SUPERPLASTICITY OF 7B04 Al SHEET[J]. 金属学报, 2015, 51(12): 1449-1456.
[6] FU Mingjie, HAN Xiuquan, WU Wei, ZHANG Jianwei. SUPERPLASTICITY RESEARCH OF Ti-23Al-17Nb ALLOY SHEET[J]. 金属学报, 2014, 50(8): 955-961.
[7] MA Pinkui, SONG Yuquan. BINOCULAR STEREO VISION MEASUREMENT RESEARCH FOR SUPERPLASTIC FREE BULGING[J]. 金属学报, 2014, 50(4): 471-478.
[8] GUAN Zhiping, MA Pinkui, SONG Yuquan. ANALYSIS OF FRACTURE DURING SUPERPLASTIC TENSION[J]. 金属学报, 2013, 49(8): 1003-1011.
[9] SHEN Jun, FENG Aihan. RECENT ADVANCES ON MICROSTRUCTURAL CONTROLLING AND HOT FORMING OF Ti2AlNb-BASED ALLOYS[J]. 金属学报, 2013, 49(11): 1286-1294.
[10] HOU Jieshan, ZHOU Lanzhang, GUO Jianting, YUAN Chao. APPLICATION OF ARTIFICIAL NEURAL NETWORK FOR PREDICTION OF SUPERPLASTIC  BEHAVIOUR IN NiAl ALLOYS[J]. 金属学报, 2013, 49(11): 1333-1338.
[11] CAO Furong DING Hua WANG Zhaodong LI Yinglong GUAN Renguo CUI Jianzhong . QUASI–SUPERPLASTICITY AND DEFORMATION MECHANISM OF ULTRALIGHT β SOLID SOLUTION Mg–11Li–3Zn ALLOY[J]. 金属学报, 2012, 48(2): 250-256.
[12] WANG Gang XU Lei WANG Yong ZHENG Zhuo CUI Yuyou YANG Rui. HOT DEFORMATION BEHAVIOR AND MICROSTRUCTURE EVOLUTION OF A HIGH-Nb-CONTAINING TiAl BASED ALLOY[J]. 金属学报, 2011, 47(5): 587-593.
[13] CAO Furong GUAN Renguo DING Hua LI Yinglong ZHOU Ge CUI Jianzhong. DISLOCATION CREEP IN SUPER–LIGHT α SOLID SOLUTION BASE Mg–6Li–3Zn ALLOY[J]. 金属学报, 2010, 46(6): 715-722.
[14] ZHANG Han BAI Bingzhe FANG Hongsheng. EFFECT OF PRESTRAIN ON THE SUPERPLASTIC DEFORMATION BEHAVIOR OF LOW-ALLOY HIGH-CARBON STEEL[J]. 金属学报, 2009, 45(9): 1106-1110.
[15] KANG Zhixin PENG Yonghui SANG Jing JIAN Weiwei ZHAO Haidong LI Yuanyuan. SUPERPLASTICITY AND MICROSTRUCTURE EVOLUTION IN Mg-1.5Mn-0.3Ce ALLOY DEFORMED BY T-SHAPE CHANNEL PRESSING[J]. 金属学报, 2009, 45(9): 1117-1124.
No Suggested Reading articles found!