| ROOM-TEMPERATURE SLIDING WEAR PROPERTIES OF LASER MELT DEPOSITED Cr13Ni5Si2/γ TERNARY METAL SILICIDE ALLOY |
| Y.L. Fang;H.M. Wang |
| 北京航空航天大学材料科学与工程学院 |
|
Cite this article:
Y.L. Fang; H.M. Wang. ROOM-TEMPERATURE SLIDING WEAR PROPERTIES OF LASER MELT DEPOSITED Cr13Ni5Si2/γ TERNARY METAL SILICIDE ALLOY. Acta Metall Sin, 2006, 42(2): 181-185 .
|
|
|
Abstract A wear resistant metal silicide alloy consisting of Cr13Ni5Si2 ternary metal silicide dendrites and the interdendritic nickel-base solid solution (γ) was designed and fabricated by the laser melting/continuous deposition process. Wear resistance of the Cr13Ni5Si2/γ alloy was evaluated on an MM-200 block-on-wheel dry sliding wear tester at room temperature. Results indicate that the Cr13Ni5Si2/γ alloy has excellent wear resistance and extremely low load-sensitivity of wear under dry sliding wear test conditions.
|
|
Received: 30 May 2005
|
|
|
[1] Hawk J A, Alman D E. Mater Sci Eng, 1997; A239-240: 899 [2] Johnson B J, Kennedy F E, Baker I. Wear, 1996; 192: 241 [3] Hawk J A, Alman D E. Wear, 1999; 225-229: 544 [4] Alman D E, Hawk J A, Tylczak J H, Dogan C P, Wilson R D. Wear, 2001; 251: 875 [5] Yang J, La P Q, Liu W M, Xue Q J. Wear, 2004; 257: 104 [6] Jin J H, Stephenson D J. Wear, 1998; 217: 200 [7] Hawk J A, Alman D E. Scr Mater, 1995; 5: 725 [8] Alman D E, Hawk J A. Wear, 2001; 251: 890 [9] Kim J H, Tabaru T, Hirai H, Kitahara A, Hanada S. Scr Mater, 2003; 48: 1439 [10] Zhou J, Guo J T. Mater Sci Eng, 2003; A339: 166 [11] Misra A, Gibala R, Noebe R D. Intermetallica, 2001; 9: 971 [12] Xu H P, Ngan A H W, Duggan B J, Chen Q Z. Mater Lett, 1997; 31: 233 [13] Mishima Y, Kato M, Kimura Y, Hosoda H, Miura S. Intermetallics, 1996; 4: 171 [14] Villars P, Prince A, Okamoto H. Handbook of Ternary Alloys Phase Diagrams. New York: ASM International, 1995: 9143 [15] Tang H B, Fang Y L, Wang H M. Acta Mater, 2004; 52: 1773 [16] Wang H M, Zhang L Y. Chin Pat, No.02121496.4, 2002(王华明,张凌云.中国发明专利,ZL02121496.4,2002) [17] Zhang L Q, Wang H M. Mater Lett, 2003; 57: 2710 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|