| Calculation on Deposited Temperature During Pulsed Bias Arc Ion Plating |
| BAI Xiao; LIN Guoqiang; DONG Chuang; WEN Lishi |
|
Cite this article:
BAI Xiao; LIN Guoqiang; DONG Chuang; WEN Lishi. Calculation on Deposited Temperature During Pulsed Bias Arc Ion Plating. Acta Metall Sin, 2004, 40(10): 1069-1073 .
|
|
|
Abstract The influencing factors and their weights on deposited
temperature have been studied in detail during pulsed bias arc
ion plating (PBAIP). Based on the model of deposited temperature
calculation in arc ion plating (AIP), and under the condition
of the rectangle substrate voltage waveforms, the input power
intensity of ion bombardment in PBAIP can be equal to the product
of the input power in AIP and duty cycle in PBAIP. On the basis of energy
conversation principle, a substrate temperature calculation model
for PBAIP is established when the bias voltage varies from -1000 V
to 0. Experiments are also used to verify the calculated results and
a good agreement is obtained.
|
|
Received: 10 October 2003
|
|
|
[1] Perry A J, Tian A F, Treglio J R, Loomics C. Surf CoatTechnol, 1994; 68-69: 528 [2] Olbrich W, Fessmann J, Kampschulte G, Ebberink J. SurfCoat Technol, 1991; 49: 258 [3] Wen L S, Huang R F. Surf Coat Technol, 1998; 14: 289 [4] Fessmann J, Olbrich W, Kampschulte G, Ebberink J.Mater Sci Eng, 1991; A140: 830 [5] Huang M D, Sun C, Lin G Q, Dong C, Wen L S. ActaMetall Sin, 2003; 39: 516(黄美东,孙超,林国强,董闯,闻立时.金属学报,2003;39:516) [6] Huang M D, Lin G Q, Dong C, Sun C, Wen L S. Acta Metall Sin, 2003; 39: 510(黄美东,林国强,董闯,孙超,闻立时.金属学报,2003;39:510) [7] Olbrich W, Kampschulte G. Surf Coat Technol, 1993; 59:274 [8] Olbrich W, Kampschulte G. Surf Coat Technol, 1993; 61:262 [9] Li Z Y, Zhu W B, Zhang Y, Li G Y, Cao E Y. Surf CoatTechnol, 2000; 131: 15 [10] Engers B, Fuchs H, Schjultz J, Hettkamp E, Mecke H. SurfCoat Technol, 2000; 133-134: 121 [11] Huang M D, Lin G Q, Dong C, Sun C, Huang R F, WenL S. Trans Mater Heat Treat, 2001; 22: 75(黄美东,林国强,董闯,孙超,黄荣芳,闻立时.材料热处理学报,2001;22:75) [12] Lin G Q, Ding Z F, Qi D, Zhao Y H, Wang N H, Dong C.J Vac Sci Technol A, 2003: 21: 1675 [13] Tang J. Electrotechnics. Beijing: Publishing Company ofHigher Education, 1999: 55(唐介.电工学.北京:高等教育出版社,1999:55) [14] Alfred G. Cold Plasma in Materials Fabrication-from Fundamentals to Applications. New York: IEEE Press, 1993: 12 [15] Ljungcrantz'H, Hultman L, Sundgren J E, Karisson L. J Appl Phys, 1995; 78: 832 [16] Brown I G. Rev Sci Instrum, 1994; 65: 3061 |
| No Suggested Reading articles found! |
|
|
Viewed |
|
|
|
Full text
|
|
|
|
|
Abstract
|
|
|
|
|
Cited |
|
|
|
|
| |
Shared |
|
|
|
|
| |
Discussed |
|
|
|
|