Please wait a minute...
Acta Metall Sin  2006, Vol. 42 Issue (5): 474-480     DOI:
Research Articles Current Issue | Archive | Adv Search |
SIMULATION OF STATIC RECRYSTALLIZATION OF HOT DEFORMED AUSTENITE IN A LOW CABON STEEL ON MESOSCALE
中国科学院金属研究所
Cite this article: 

. SIMULATION OF STATIC RECRYSTALLIZATION OF HOT DEFORMED AUSTENITE IN A LOW CABON STEEL ON MESOSCALE. Acta Metall Sin, 2006, 42(5): 474-480 .

Download:  PDF(1303KB) 
Export:  BibTeX | EndNote (RIS)      
Abstract  Based on the distribution of stored energy in hot deformed austenite simulated by a crystal plasticity finite element method (CPFEM), the static recrystallization of a low carbon steel was investigated by a 2D cellular automaton (CA) model on mesoscale. The effect of the inhomogeneous distribution of the stored energy on the static recrystallization was simulated, which was difficult for the traditional recrystallization CA models. The simulated results revealed that the density of recrystallization nucleation varied in different sites due to the inhomogeneous distribution of stored energy, and the nuclei concentrated both at the grain boundary and in the heavily deformed grain interiors. The number of recrystallized nuclei increased and the distribution of the nucleation inclined to homogeneity with the decreased critical stored energy for nucleation. In addition, the recrystallization kinetics under various nucleation criteria was discussed in the present paper.
Key words:  crystal plasticity finite element model      stored energy      cellular automaton      static recrystallization      
Received:  29 November 2005     
ZTFLH:  TG111.7  
Service
E-mail this article
Add to citation manager
E-mail Alert
RSS
()
Articles by authors

URL: 

https://www.ams.org.cn/EN/     OR     https://www.ams.org.cn/EN/Y2006/V42/I5/474

[1] Raabe D. Computational Materials Science. Weinheim: Wiley-VCH , 1998: 201
[2] Hesselbarth H W, Gobel I R. Acta Metall Mater, 1991; 39: 2135
[3] Marx V, Reher F R, Gottstein G. Acta Mater, 1999; 47: 1219
[4] Raabe D. Ann Rev Mater Res, 2002; 32: 53
[5] Goetz R L, Seetharaman V. Metall Mater Trans, 1998; 29A: 2307
[6] Ding R, Guo Z X. Acta Mater, 2001; 49: 3163
[7] Kroc J. Lect Note Comp Sci, 2002; 2329: 773
[8] Kugler G, Turk R. Acta Mater, 2004; 52: 4659
[9] Sun J H, Liu Y Z, Zhou L Y. Spec Steel, 2004; 25: 12 (孙景宏,刘雅政,周乐育.特殊钢,2004;25:12)
[10] Dewri R, Chakraborti N. Model Simul Mater Sci Eng, 2005; 13: 173
[11] Doherty R D, Hughes D A, Humphreys F J, Jonas J J, Jensen D J, Kassner M E, King W E, McNelley T R, McQueen H J, Rollett A D. Mater Sci Eng, 1997; A238: 219
[12] Solas D E, Tome C N, Engler O, Wenk H R. Acta Mater, 2001: 49: 3791
[13] Choi S H, Cho J H. Mater Sci Eng, 2005; A405: 86
[14] Hill R, Rice J R. J Int Phys Solids, 2004; 20: 339
[15] Radhakrishnan B, Sarma G B, Zacharia T. Acta Mater, 1998; 46: 4415
[16] Raabe D, Becker R C. Model Simul Mater Sci Eng, 2000; 8: 445
[17] Humphreys F J. Mater Sci Forum, 2004; 467-470: 107
[18] Song X Y, Rettenmayr M, Muller C, Exner H E. Metall Mater Trans, 2001; 32A: 2199
[19] Davies C H J. Scr Mater, 1997; 36: 35
[20] Hutchinson W B. Int Met Rev, 1984; 29: 25
[21] Tong M M, Mo C L, Li D Z, Li Y Y. Chin J Mater Res, 2002; 16: 485 (佟铭明,莫春立,李殿中,李依依.材料研究学报,2002;16: 485)
[22] Read W T, Shockley W. Phys Rev, 1950; 78: 275
[23] Hibbitt, Karlsson and Sorensen. Abaqus/Standard User's Manual, Vol.3, Pawtucket, RI, USA, 1999: 24.2.30-1
[24] Xiao N M, Yue Z F, Lan Y J, Tong M M, Li D Z. Acta Metall Sin, 2005; 41: 496 (肖纳敏,岳珠峰,兰勇军,佟铭明,李殿中.金属学报,2005; 41:496)
[25] Lan Y J, Xiao N M, Li D Z, Li Y Y. Acta Mater, 2005; 53: 991
[26] Rollett A D. Prog Mater Sci, 1997; 42: 79
[27] Rios P R, Padilha A F. Mater Res, 2003; 6: 605
[28] Rollett A D, Srolovitz D J, Doherty R D, Anderson M P. Acta Metall Mater, 1989; 37: 627
[1] Jialin ZHU,Shifeng LIU,Yu CAO,Yahui LIU,Chao DENG,Qing LIU. Effect of Cross Rolling Cycle on the Deformed and Recrystallized Gradient in High-Purity Tantalum Plate[J]. 金属学报, 2019, 55(8): 1019-1033.
[2] Hui FANG,Hua XUE,Qianyu TANG,Qingyu ZHANG,Shiyan PAN,Mingfang ZHU. Dendrite Coarsening and Secondary Arm Migration in the Mushy Zone During Directional Solidification:[J]. 金属学报, 2019, 55(5): 664-672.
[3] Mingfang ZHU, Like XING, Hui FANG, Qingyu ZHANG, Qianyu TANG, Shiyan PAN. Progresses in Dendrite Coarsening During Solidification of Alloys[J]. 金属学报, 2018, 54(5): 789-800.
[4] Tongmin WANG, Jingjing WEI, Xudong WANG, Man YAO. Progress and Application of Microstructure Simulation of Alloy Solidification[J]. 金属学报, 2018, 54(2): 193-203.
[5] Lei WEI, Yongqing CAO, Haiou YANG, Xin LIN, Meng WANG, Weidong HUANG. Numerical Simulation of Anomalous Eutectic Growth of Ni-Sn Alloy Under Laser Remelting of Powder Bed[J]. 金属学报, 2018, 54(12): 1801-1808.
[6] Mingfang ZHU, Qianyu TANG, Qingyu ZHANG, Shiyan PAN, Dongke SUN. CELLULAR AUTOMATON MODELING OF MICRO-STRUCTURE EVOLUTION DURING ALLOY SOLIDIFICATION[J]. 金属学报, 2016, 52(10): 1297-1310.
[7] Rui CHEN, Qingyan XU, Qinfang WU, Huiting GUO, Baicheng LIU. NUCLEATION MODEL AND DENDRITE GROWTH SIMULATION IN SOLIDIFICATON PROCESS OF Al-7Si-Mg ALLOY[J]. 金属学报, 2015, 51(6): 733-744.
[8] ZHANG Lei, ZHAO Honglei, ZHU Mingfang. SIMULATION OF SOLIDIFICATION MICROSTRUC-TURE OF SPHEROIDAL GRAPHITE CAST IRON USING A CELLULAR AUTOMATON METHOD[J]. 金属学报, 2015, 51(2): 148-158.
[9] ZHAO Jiuzhou, LI Lu, ZHANG Xianfei. DEVELOPMENT OF CELLULAR AUTOMATON MODELS AND SIMULATION METHODS FOR SOLIDIFICATION OF ALLOYS[J]. 金属学报, 2014, 50(6): 641-651.
[10] DAI Qilei, LIANG Zhifang, WU Jianjun, MENG Lichun, SHI Qingyu. MICROSTRUCTURE CHANGE AND ENERGY RELEASE OF FRICTION STIR WELDED Al-Mg-Si ALLOY DURING DSC TEST[J]. 金属学报, 2014, 50(5): 587-593.
[11] LI Zhengyang, ZHU Mingfang, DAI Ting. MODELING OF MICROPOROSITY FORMATION IN AN Al-7%Si ALLOY[J]. 金属学报, 2013, 49(9): 1032-1040.
[12] HUANG Hongtao Godfrey Andrew LIU Wei TANG Ruihe LIU Qing. EFFECT OF SAMPLE ORIENTATION ON STATIC RECRYSTALLIZATION OF AZ31 MAGNESIUM ALLOY[J]. 金属学报, 2012, 48(8): 915-921.
[13] . EFFECT OF FORCED FLOW ON THREE DIMENSIONAL DENDRITIC GROWTH OF Al-Cu ALLOYS[J]. 金属学报, 2012, 48(5): 615-620.
[14] GANG Jianwei,SHI Binqing, CHEN Rongshi, KE Wei. MICROSTRUCTURE EVOLUTION AND STATIC RECRYSTALLIZATION BEHAVIOR OF HOT-ROLLED Mg-1Zn AND Mg-1Y ALLOYS DURING ISOTHERMAL ANNEALING[J]. 金属学报, 2012, 48(5): 526-533.
[15] SHI Yufeng XU Qingyan LIU Baicheng. SIMULATION OF EUTECTIC GROWTH IN DIRECTIONAL SOLIDIFICATION BY CELLULAR AUTOMATON METHOD[J]. 金属学报, 2012, 48(1): 41-48.
No Suggested Reading articles found!